Hardfacing of metal parts employing a thin, homogeneous ductile foil is disclosed. The hardfacing foil has a composition consisting essentially of about 0 to about 25 atom percent cobalt, 0 to about 30 atom percent nickel, 0 to about 30 atom percent chromium, 0 to about 5 atom…
Bose Debasis
Apparatus is provided for fabricating continuous metal strip composed of a low density, readily oxidizable aluminum based alloy. The allow is cast directly from the melt through a slotted nozzle onto a moving chill substrate. A scraping mechanism located upstream of the nozzle…
Apparatus is provided for fabricating continuous metal strip composed of a low density, readily oxidizable aluminum based alloy. The alloy is cast directly from the melt through a slotted nozzle onto a moving chill substrate. A scraping mechanism located upstream of the nozzle…
A nickel based high melting point, homogeneous, ductile brazing foil composition consists essentially of about 17 to 20 atom percent chromium, about 4 to 10 atom percent boron, about 10 to 16 atom percent silicon, the balance being nickel and incidental impurities. The…
A copper based low melting point metal alloy composition consists essentially of about 2.5 to 11 atom percent tin, about 0 to 12 atom percent nickel and about 11 to 15 atom percent boron, the balance being essentially copper and incidental impurities. The composition is such…
A copper based low melting point metal alloy composition consists essentially of about 5 to 52 atom percent nickel, about 2 to 10 atom percent tin, about 10 to 15 atom percent phosphorus and the balance essentially copper and incidental impurities. The composition is such that…
A nickel based metal alloy consists essentially of about 25 to 35 atom percent palladium and about 15 to 20 atom percent silicon the balance being essentially nickel and incidental impurities. The alloy is especially suited for use as a filler metal in joining steels and…
Brazing of metal parts employing a low temperature, high strength metal alloy is disclosed. The alloy has a composition consisting essentially of about 6.10 to 6.66 atom percent chromium, about 2.43 to 2.46 atom percent iron, about 10.06 to 25.10 atom percent boron, about 3.22…
A nickel based high melting homogeneous, ductile brazing foil composition consists essentially of 17 to 20 atom percent chromium, 4 to 10 atom percent boron, 10 to 16 atom percent silicon, the balance being nickel and incidental impurities. The composition is such that the total…
A copper based low melting point metal alloy composition consists essentially of about 10 to 52 atom percent nickel, about 2 to 10 atom percent tin, about 10 to 15 atom percent phosphorus and the balance essentially copper and incidental impurities. The composition is such that…
A nickel based metal alloy consists essentially of about 25 to 35 atom percent palladium and about 15 to 20 atom percent silicon the balance being essentially nickel and incidental impurities. The alloy is especially suited for use as a filler metal in joining steels and…
A lead based, tin free alloy is modified by adding thereto about 0.5 to 4 weight percent of tin. The alloy is rapidly solidified by forming a melt thereof containing the tin addition and quenching the melt on a moving chill surface at a quenching rate of at least about 105 DEG…
A lead based alloy is modified by adding thereto a surfactant consisting of about 0.01 to 0.5 weight percent tellurium, about 0.01 to 0.5 weight percent selenium, about 0.01 to 0.5 weight percent selenium plus about 0.1-0.5 weight percent antimony, and mixtures thereof. The…
Hardfacing of metal parts employing a thin, homogeneous ductile foil is disclosed. The hardfacing foil has a composition based on a metal selected from the group consisting of iron, cobalt and nickel. The ductile foil permits continuous hardfacing of soft matrix, like low carbon…
A copper based low melting point metal alloy composition consists essentially of about 5 to 52 atom percent nickel, about 2 to 10 atom percent tin, about 10 to 15 atom percent phosphorus and the balance essentially copper and incidental impurities. The composition is such that…
A rapidly solidified, homogeneous soldering foil has a thickness ranging from 12 to 200 micrometers. The foil is at least 2 millimeters wide, of substantially uniform cross section along its length and has a composition consisting essentially of at least two elements selected…
Apparatus is provided for fabricating continuous metal strip composed of a low density, readily oxidizable aluminum based alloy. The alloy is cast directly from the metal through a slotted nozzle onto a moving chill substrate. A scraping mechanism located upstream of the nozzle…
A low melting aluminum brazing alloy of about 15-25 wt. percent silver, about 15-25 wt. percent copper, about 1-5 wt. percent silicon, about 0-3 wt. percent zinc, about 0-2 wt. percent magnesium, about 0-2 wt. percent iron and the balance essentially aluminum and incidental…
Hardfacing of metal parts employing a thin, homogeneous, ductile foil is disclosed. The hardfacing foil has a composition consisting essentially of 0 to about 25 atom percent cobalt, 0 to about 20 atom percent iron, 0 to about 15 atom percent chromium, 0 to about 16 atom percent…
Brazing of metal parts employing a low temperature, high strength metal alloy is disclosed. The alloy has a composition consisting essentially of about 10 to 30 atom percent palladium, about 5 to 20 atom percent chromium, about 1 to 5 atom percent of at least one metal selected…
A process of brazing using a copper based low melting point metal alloy composition consisting essentially of about 2.5 to 11 atom percent tin and about 11 to 15 atom percent boron, the balance being essentially copper and incidental impurities. The composition is such that the…
Hardfacing of metal parts employing a thin, homogeneous ductile foil is disclosed. The hardfacing foil has a composition consisting essentially of about 0 to about 25 atom percent cobalt, 0 to about 30 atom percent nickel, 0 to about 30 atom percent chromium, 0 to about 5 atom…
A nickel based high melting point, homogeneous, ductile brazing foil composition consists essentially of about 17 to 20 atom percent chromium, about 4 to 10 atom percent boron, about 10 to 16 atom percent silicon, the balance being nickel and incidental impurities. The…
A copper based low melting point metal alloy composition consists essentially of about 2.5 to 11 atom percent tin and about 11 to 15 atom percent boron, the balance being essentially copper and incidental impurities. The composition is such that the total of copper and tin…
Hardfacing of metal parts employing a thin, homogeneous, ductile foil is disclosed. The hardfacing foil has a composition consisting essentially of 0 to about 32 atom percent nickel, 0 to about 10 atom percent iron, 0 to about 30 atom percent chromium, 0 to about 2 atom percent…