Patents
Inventor / Author Profile

Boardman Harold

62Total Forward Citations
16Indexed Patents
4Patent H-Index
US 3,924,520 A#3354697 Most Cited · 23 citations0.5/yr · PR 6.21ExpiredUS · Utility
Preparing lithographic plates utilizing vinyl monomers containing hydrolyzable silane groups
Inventors: Boardman Harold, Breslow David S, Simpson David A, Wagner Richard LAssignee: Hercules IncFiled 1974-06-27 · Granted 1975-12-09

It has been found that photopolymer elements, particularly lithographic printing plates, can be prepared by (a) treating the surface of a polymer film with a photooxygenation sensitizer, said film being a film of a polymer containing extralinear olefinic unsaturation of the type…

US 3,905,816 A#7366083 Most Cited · 13 citations0.2/yr · PR 3.25ExpiredUS · Utility
Preparing lithographic plates utilizing hydrolyzable azoand azido-silane compounds
Inventors: Boardman Harold, Wagner Richard LAssignee: Hercules IncFiled 1974-06-27 · Granted 1975-09-16

It has been found that lithographic printing plates can be prepared by (a) photografting to an oleophilic organic polymer substrate a potentially hydrophilic hydrolyzable azo- or azidosilane compound having the general formula WHERE R is an organic radical, X is selected from…

US 3,907,564 A#8800893 Most Cited · 11 citations0.2/yr · PR 4.72ExpiredUS · Utility
Preparing lithographic plates utilizing hydrolyzable mercapto-silane compounds
Inventors: Boardman Harold, Wagner Richard LAssignee: Hercules IncFiled 1974-06-27 · Granted 1975-09-23

It has been found that lithographic printing plates can be prepared by (a) photografting to an unsaturated oleophilic organic polymer substrate a potentially hydrophilic hydrolyzable mercapto-silane compound having the general formula WHERE R is an organic radical, X is selected…

GB 781,040 A#36234268 Most Cited · 2 citations0.0/yr · PR 1.19ExpiredGB · Utility
Improvements in or relating to the preparation of vulcanized natural or synthetic rubber products
Inventors: Boardman HaroldAssignee: Hercules Powder Co LtdFiled 1955-09-22

Synthetic rubber is vulcanized by heating with 0.1 to 10 per cent based on the weight of rubber of a peroxide of the formula <FORM:0781040/IV (a)/1> where R1 is an aryl group and R2, R3, R4, R5, and R6 are selected from hydrogen and alkyl groups of less than 4 carbon…