US 5,750,605 A#1353730 Most Cited · 41 citations1.5/yr · PR 4.40ExpiredUS · Utility
Hot melt adhesives based on sulfonated polyesters
Inventors: Blumenthal Mitchell J, Sharak Matthew L, Paul Charles WAssignee: Nat Starch Chem InvestFiled 1996-05-23 · Granted 1998-05-12

A hot melt adhesive composition comprising (i) 10 to 90% by weight of a sulfonated polyester condensation polymer; (ii) 0 to 80% by weight of a compatible tackifier; (iii) 0 to 40% by weight of a compatible plasticizer; (iv) 5 to 40% by weight of a compatible wax diluent with a…

US 6,653,522 B1#1774220 Most Cited · 35 citations1.5/yr · PR 4.32ExpiredUS · Utility
Hot melt adhesives based on sulfonated polyesters comprising wetness indicator
Inventors: Blumenthal Mitchell J, Paul Charles WAssignee: Nat Starch Chem InvestFiled 1999-04-09 · Granted 2003-11-25

A wetness indicating hot melt adhesive composition comprising a pH adjusting component and an indicating agent which is capable of changing color in response to changes in pH. The adhesive composition may comprise 20 to 80% by weight of a sulfonated polyester, 3 to 30% by weight…

EP 0,761,795 A2#3908603 Most Cited · 21 citations0.7/yr · PR 3.87PendingEP · Application
Hot melt adhesives based on sulfonated polyesters

A hot melt adhesive composition comprising (i) 10 to 90% by weight of a sulfonated polyester; condensation polymer comprising the reaction product of a) at least one difunctional dicarboxylic acid or the corresponding methyl ester which is not a sulphomonomer; b) 2 to 25 mole…

US 6,001,910 A#4280339 Most Cited · 20 citations0.7/yr · PR 2.87ExpiredUS · Utility
Use of anionic or cationic plasticizers with sulfonated polyesters in hot melt formulations
Inventors: Blumenthal Mitchell J, Paul Charles W, Sharak Matthew LAssignee: Nat Starch Chem InvestFiled 1999-04-09 · Granted 1999-12-14

A remoistenable hot melt adhesive composition comprising (i) 25 to 80% by weight of a sulfonated polyester; (ii) 3 to 40% by weight of an anionic or cationic plasticizer; (iii) 0 to 40% by weight of a polar tackifier; (iv) 0 to 3% by weight of an antioxidant; and (v) 10 to 35%…

EP 1,043,377 A2#6138878 Most Cited · 15 citations0.6/yr · PR 3.60PendingEP · Application
Hot melt adhesives based on sulfonated polyesters comprising wetness indicator
Inventors: Blumenthal Mitchell J, Paul Charles WAssignee: Nat Starch Chem InvestFiled 2000-04-10

A wetness indicating hot melt adhesive composition comprising a pH adjusting component and an indicating agent which is capable of changing color in response to changes in pH. The adhesive composition may comprise 20 to 80 % by weight of a sulfonated polyester, 3 to 30% by…

US 6,410,627 B1#7086606 Most Cited · 14 citations0.6/yr · PR 1.98ExpiredUS · Utility
Use of high hydroxyl compounds for water sensitive hot melt adhesives
Inventors: Paul Charles W, Blumenthal Mitchell JAssignee: Nat Starch Chem InvestFiled 1999-04-09 · Granted 2002-06-25

A hot melt adhesive composition comprising (a) greater than 40% by weight of a polymeric component; and (b) 5 to 40% by weight of a high hydroxyl number compound, with hydroxyl number greater than 100 mg KOH/g.

US 2004220308 A1#7480044 Most Cited · 13 citations0.6/yr · PR 2.79PendingUS · Application
Labeling adhesive

The use of dimer acids with conventional hot melt adhesive polymers provide adhesives particularly useful for bottle labeling. The label, along with the adhesive, can be easily removed from the bottle during the recycling process.

US 7,109,263 B2#12074580 Most Cited · 9 citations0.5/yr · PR 1.71ExpiredUS · Utility
Labeling adhesive
Inventors: Paul Charles W, Blumenthal Mitchell, Willis LineAssignee: Nat Starch Chem InvestFiled 2003-05-02 · Granted 2006-09-19

The use of dimer acids with conventional hot melt adhesive polymers provide adhesives particularly useful for bottle labeling. The label, along with the adhesive, can be easily removed from the bottle during the recycling process.

US 2006235122 A1#12844509 Most Cited · 8 citations0.4/yr · PR 2.28PendingUS · Application
Labeling adhesive

The use of dimer acids with conventional hot melt adhesive polymers provide adhesives particularly useful for bottle labeling. The label, along with the adhesive, can be easily removed from the bottle during the recycling process.

JP 2001011425 A#14971807 Most Cited · 7 citations0.3/yr · PR 1.90ExpiredJP · Utility
Hot-melt adhesive based on sulfonated polyester containing wetness indicator
Inventors: Blumenthal Mitchell J, Paul Charles WAssignee: Nat Starch Chem InvestFiled 2000-04-07

PROBLEM TO BE SOLVED: To provide a hot-melt adhesive which indicates the presence of water or urine and a disposable product containing the adhesive. SOLUTION: A hot-melt adhesive which indicates wetness contains a pH adjuster component and an indicator which discolors in…

US 6,174,988 B1#14509882 Most Cited · 7 citations0.3/yr · PR 2.31ExpiredUS · Utility
Use of polyamino acid salts in water-borne adhesive applications
Inventors: Guth Jacob J, Lad Niketa S, Iovine Carmine, Blumenthal MitchellAssignee: Nat Starch & Chemical CompanyFiled 1999-04-07 · Granted 2001-01-16

This invention relates to an adhesive composition which comprises (a) an adhesive carrier, and (b) an adhesively effective amount of a polyamino acid salt selected from the group consisting of polyaspartic acid salts, polyglutamic acid salts, and copolymers of polyaspartic acid…

EP 1,046,691 A2#22571536 Most Cited · 4 citations0.1/yr · PR 3.72PendingEP · Application
Use of high hydroxyl compounds for water sensitive hot melt adhesives
Inventors: Blumenthal Mitchell J, Paul Charles WAssignee: Nat Starch Chem InvestFiled 2000-04-10

A hot melt adhesive composition comprising (a) greater than 40% by weight of a polymeric component; and (b) 5 to 40% by weight of a high hydroxyl number compound, with hydroxyl number greater than 100 mg KOH/g.

CA 2,184,743 A1#32743472 Most Cited · 3 citations0.1/yr · PR 1.08PendingCA · Application
Hot melt adhesives based on sulfonated polyesters

A hot melt adhesive composition comprising (i) 10 to 90% by weight of a sulfonated polyester; condensation polymer comprising the reaction product of a) at least one difunctional dicarboxylic acid or the corresponding methyl ester which is not a sulphomonomer; b) 2 to 25 mole…

CA 2,367,297 A1#31282590 Most Cited · 3 citations0.1/yr · PR 1.16PendingCA · Application
Use of polyamino acid salts in water-borne adhesive applications

This invention relates to an adhesive composition which comprises (a) an adhesive carrier, and (b) an adhesively effective amount of a polyamino acid salt selected from the group consisting of polyaspartic acid salts, polyglutamic acid salts, and copolymers of polyaspartic acid…

WO 0,059,985 A1#37728338 Most Cited · 2 citations0.1/yr · PR 1.09PendingWO · Application
Use of polyamino acid salts in water-borne adhesive applications

This invention relates to an adhesive composition which comprises (a) an adhesive carrier, and (b) an adhesively effective amount of a polyamino acid salt selected from the group consisting of polyaspartic acid salts, polyglutamic acid salts, and copolymers of polyaspartic acid…

JP 2001011417 A#54458177 Most Cited · 1 citations0.0/yr · PR 0.81ExpiredJP · Utility
Use of sulfonated polyester and anionic or cationic plasticizer in hot-melt blend

PROBLEM TO BE SOLVED: To provide a remoistening hot-melt adhesive having an excellent blocking resistance in a high-temperature high-humidity environment. SOLUTION: A remoistening hot-melt adhesive composition contains (i) 25 to 80 wt.% sulfonated polyester, (ii) 3 to 40 wt.%…

CA 2,304,867 A1#102726537 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Use of anionic or cationic plasticizers with sulfonated polyesters in hot melt formulations

A remoistenable hot melt adhesive composition comprising (i) 25 to 80% by weight of a sulfonated polyester; (ii) 3 to 40% by weight of an anionic or cationic plasticizer; (iii) 0 to 40% by weight of a polar tackifier; (iv) 0 to 3% by weight of an antioxidant; and (v) 10 to 35%…

EP 1,043,376 A2#150460858 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Use of anionic or cationic plasticizers with sulfonated polyesters in hot melt formulations

A remoistenable hot melt adhesive composition comprising (i) 25 to 80% by weight of a sulfonated polyester; (ii) 3 to 40% by weight of an anionic or cationic plasticizer; (iii) 0 to 40% by weight of a polar tackifier; (iv) 0 to 3% by weight of an antioxidant; and (v) 10 to 35%…