The present invention is concerned with thermoplastic terephthalic acid copolyesters which crystallize more rapidly than homopolyethylene terephthalate and are based on a diol component which is about 98 to 99.9 mol % of ethylene glycol and the balance 2-ethylhexane-1,3-diol.…
Gepfropfte Polyacrylate bestimmter Zusammensetzung verbessern die mehraxiale Schlagzähigkeit thermoplastischer Polyester.
The toughness of polybutylene terephthalate can be considerably improved by the addition of an ABS-graft copolymer having a relatively high content of graft base and a closely defined particle size; the typical properties of polybutylene terephthalate, such as its high…
Terephthalic copolyesters, the diol component of which consists of ethylene glycol and 2.2-diethyl propane-1.3-diol crystallize more rapidly than pure polyethylene terephthalate and can be molded in a way comparable to butylene terephthalate.
The heat distortion resistance and the molecular weight of polypropylene terephthalate and polybentylene terephthalate can be increased by cocondensing up to 10 mol-% of aliphatic diols containing 5 to 10 carbon atoms or of cycloaliphatic diols containing 8 to 12 carbon atoms.
Grafted polyacrylates having a specific composition improve the impact strength under multi-axial stress of thermoplastic polyesters.
This invention relates to polyalkylene terephthalates which crystallize rapidly, and process of making such compositions and a process of using such compositions in injection molding. The compositions comprise polyalkylene terephthalates with intrinsic viscosities in excess of…
The present invention relates to thermoplastic moulding compositions, which have improved impact strength at low temperature, comprising thermoplastic polyesters, in particular polyalkylene terephthalates, and grafted, partially or highly cross-linked diene rubbers and/or…
The present invention is concerned with mixtures of branched polyaryl-sulphone and aromatic polycarbonates having Mw in excess of about 60,000. These mixtures are particularly suitable for the production of extruded film although the polycarbonate itself is of too high a…
Terephthalic copolyesters, the diol component of which mainly consists of ethylene glycol units, crystallize more rapidly than pure polyethylene terephthalate and can be moulded in a way comparable to polybutylene terephthalate.
Polyalkylene terephthalates containing 0.5-30% by weight of oligomeric carboxylic acid polyesters have a higher crystallization speed and thus allow lower mold temperatures and shorter injection cycles. The polyalkylene terephthalates generally have intrinsic viscosities in…
Copolymers of (a) one or more α-olefins having the formula (A) ##STR1## wherein R is a C 1 -C 16 alkyl group or a phenyl group; and (b) one or more substituted α-olefins having the formula (B) ##STR2## wherein R 1 is a hydrogen atom or a methyl group, R 2 is a hydrogen atom or a…
The present invention is concerned with polycarbonate molding resins with improved flow and strength properties which contain about 10 to 40 wt.% glass fibers and about 0.5 to 5 wt. % of polyalkylene glycol terephthalate or about 0.5 to 10 wt.% of polyalkylene glycol…
Moulding compositions of aromatic polycarbonate, polyalkylene terephthalate and a certain graft copolymer which may be processed into mouldings characterized by high multiaxial impact strength, exhibit an increased Vicat B-temperature if they contain a low amount of an ethylene…
Polyalkylene terephthalates containing 0.5-30% by weight of monomeric aliphatic carboxylic acid esters have a higher crystallization speed and thus allow lower mold temperatures and shorter injection cycles. The polyalkylene terephthalates generally have intrinsic viscosities in…
A branched, high molecular-weight polyaryl-ether sulphone which is the reaction product of approximately equimolar amounts of an aromatic dialkali metal bishydroxylate and a bis-(halogen-aryl) compound, whose aryl nuclei are linked by sulphonyl groups, and about 0.01 to about 2…
A process for the production of modified polypropylene particles by polymerizing vinyl monomers in aqueous suspension wherein (a) an aqueous suspension is prepared which, based on 100 to 2000 parts by weight of water, contains 100 parts by weight of polypropylene particles, 4 to…
A thermoplastic mixture comprising (A) from 2 to 40% by weight of a partially crystalline ethylene/propylene copolymer or terpolymer having an ethylene content of from 70 to 90% by weight and an endothermic heat of fusion of from 6 to 18 cal/g, (B) from 30 to 93% by weight of a…
Reinforced polyamide moulding blends with improved impact strength containing as modifying agent a graft product consisting of a polyolefine as graft-substrate and grafted units of unsaturated carboxylic acids and/or derivatives therefrom and which graft product is prepared by a…
The current invention is concerned with block copolyesters of low glass transition temperature segments and ethylene glycol based polyester segments linked together by carboxylic acid ester groups and special diols, and a process for preparing these copolyesters. These…
This invention relates to thermoplastic molding compositions having improved impact strength at low temperatures comprising polyamides and grafted, at least partially crosslinked diene rubbers and/or acrylate rubbers having a bimodal rubber particle size distribution.
A process for the production of high molecular weight low color polyethylene terephthalates using a particulaarly effective polycondensation catalyst is disclosed. Titanium tetrabutylate is added to the reaction mixture after the initial esterification or transesterification…
An asymmetric semipermeable membrane of a homo- or co-polybenz-1,3-oxazine dione-(2,4).
Terephthalic copolyesters, the diol component of which mainly consists of ethylene glycol units, crystallize more rapidly than pure polyethylene terephthalate and can be moulded in a way comparable to polybutylene terephthalate.