The invention relates to tantalum powders poor in alkali and fluorine having a primary particle size of between 150 and 300 nm and a secondary particle size, defined by sintering of the primary particles, of more than 5 mu m. By sintering said tantalum powders at 1,200 DEG C for…
Inventor / Author Profile
Biermann H
29Total Forward Citations
4Indexed Patents
1Patent H-Index
Frequent Co-Inventors: Biermann H P Bott A Heine H Leitner L Naumann R Reichert K Steinberger H Wolf R
The present invention relates to a tantalum powder containing little alkali metal and fluorine, having an initial particle size of 150 to 300nm, a secondary particle size of 5 μm or more obtained by sintering the initial particles, a specific charge of a capacitor obtained by…