High temp.-resistant, flexible screen-printing ink contains, as binder, a thermoplastic aromatic polycarbonate (PC) with a Mw of at least 10,000, contg. bifunctional carbonate units of formula (I), together with halogen-free solvent(s); R<1>,R<2>=H, halo, 1-8C alkyl,…
Bier Peter Dr
Plastic laminate with a thickness of 0.2-20 mm (I) comprises: (1) a sheet of thermoplastic with a thickness of 0.02-8 mm; (2) a colour layer with a softening temp above that of (1); (3) opt a layer of polyurethane (PU) which is not sticky at room temp; and (4) a layer of…
1. Mixtures of A. 65-99% by weight of polyalkylene terephthalate, wich in turn consists of a) 1-100, preferably 10-80, in particular 30-60% by weight of polyethylene terephthalate and b) 99-0, preferably 90-20, in particular 70-40% by weight of polybutylene terephthalate, and B.…
Die Erfindung betrifft ein faserverstärktes thermoplastisches Halbzeug aus einem thermoplastisch verarbeitbaren Polymeren und langen, ein zusammenhängendes Gerüst bildenden einzelnen Verstärkungsfasern, das sich in Stanzpressen zu Formteilen mit sehr guter Oberflächenqualität…
Highly crystalline, rapidly crystallising thermoplastic compositions comprising polyphenyl sulphides and carboxylic acid esters.
The prodn. of aromatic polycarbonates (PC) with UV-absorber end-gps. and a mean M2 of 1500-150,000, opt. mixed with known aromatic PC with a similar range of M2, from diphenols, 0.001-1 mole chain cleavage agent (to 1 mole diphenol), a source of carbonic acid and opt. a chain…
Mixts. contain (A) 80-99 wt.% thermoplastic aromatic polycarbonate with a mean molecular wt. (Mw) of at least 10,000, pref. 20,000-300,000, contg. bifunctional carbonate units of formula (I); and (B) 1-20 wt.% of a terpolymer of 60-70 wt.% ethylene, 37-20 wt.% (2-12C alkyl)…
The prodn. of UV-stable polycarbonates comprises reacting thermoplastic aromatic polycarbonates of mol.wt. (Mw) 1500-250,000 (PC) with 0.01-35 wt.% of cpds. of formula (I) and 0.5-1.5 mole diaryl carbonate (per 1 mole PC) for a few mins. to a few hrs. at 200-420 degrees C and…
A process for the coating of polycarbonate mouldings made from a polycarbonate (PC) based on a diphenol of formula (Ia) comprises applying a silicone varnish with a viscosity of 5-10000 mPa.s (II) in a layer 2-200 mu m thick to the PC surface and then hardening for less than 20…
Formmassen auf Basis von Polyethylenterephthalat, Flammschutzmittel und eines bestimmten Pfropfpolymerisats zeigen eine verminderte Tropfneigung im Brandfall.
The masses contain pyrogenic silica and a polymer which reacts with polyethylene terephthalate at above 260 DEG C with crosslinking, and have an extremely good behaviour in the event of fire.
Coated mouldings of thermoplastic aromatic polycarbonate (TPC) are claimed, in which the coating itself (A) consists of TPC with a thickness of 1-200 microns, contg. 4-20 wt.% of a cpd. of formula (I), R<1> = 18-30C alkyl; R<2> = H or 1-12C alkyl. Also claimed are…
1. Process for the production of crystalline polyethylene terephthalate mouldings by injection moulding at mould temperatures of 80 to 120 degrees C, preferably 80 to 110 degrees C, characterized in that moulding compositions containing I. 70 to 98 % by weight of a polyethylene…
The polymer mixtures contain specific thermoplastic polycarbonates based on tetraalkylated diphenols, specific aromatic phosphate esters and optionally tetrafluoroethylene polymers in combination with styrene polymers and/or graft polymers.
1. Impact-resistant, crack-resistant and free-flowing polyarylene sulphide injection moulding compounds containing I. 40 to 98 parts by weight of a polyarylene sulphide having a melt viscosity of at least 5 Pas (measured at 306 degrees C and a shear stress of 10**2 Pa), II. 2 to…
Epoxy gp-contg. siloxanes of formula (I) are new: A = 1-20C alkyl with epoxy gps.; B = R1 or A; R1, R2 = 1-20C alkyl or 6-10C aryl; a, b = 0 or 1-100; and c = 1-5. Also claimed are mixts. of aromatic polycarbonates and siloxanes (I) contg. 0.001-2.5 wt.% (I).
In order to improve the adhesion of coatings, especially metal coatings, to the surfaces of plastic components, the latter are pretreated in low-pressure plasma with a process gas containing sulphur hexafluoride (SF6) which is substantially free of oxygen, the plastic surfaces…
1. Use of thermoplastic polyethylene terephthalate moulding compositions containing I. 80 to 97 % weight of a polyethylene terephthalate having an intrinsic viscosity of at least 0.3 dl/g [measured as a 0.5 % by weight solution in phenol/tetrachloroethane (weight ration 1:1) at…
1. A process for the production of materials with shear-sensitive inserts, the inserts being introduced into one at least plastic material in a screw extruder, characterized in that, at introduction of the inserts into the plastics material, all the following screw sections are…