US 5,352,542 A#3229306 Most Cited · 24 citations0.8/yr · PR 3.79ExpiredUS · Utility
Use of silver alloys as cadium-free brazing solder
Inventors: Voelcker Alexander, Beuers Joerg, Joensson Sigurd, Kaufmann Dieter, Ptaschek GeorgAssignee: DegussaFiled 1993-09-01 · Granted 1994-10-04

Cadmium-free brazing solders which also have working temperatures under 630° C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

US 5,531,962 A#11379360 Most Cited · 9 citations0.3/yr · PR 2.38ExpiredUS · Utility
Cadmium-free silver alloy brazing solder, method of using said solder, and metal articles brazed with said solder
Inventors: Weise Wolfgang, Voelcker Alexander, Kaufmann Dieter, Malikowski Willi, Beuers JoergAssignee: DegussaFiled 1994-08-03 · Granted 1996-07-02

Cadmium-free brazing solders with working temperatures under 630° C. containing 45 to 80 wt. % silver, 14 to 25 wt. % copper 10 to 25 wt. % gallium, 1 to 7 wt. % zinc and 0 to 5 wt. % indium and/or tin. The alloys have good cold workability and ductility.

US 5,341,981 A#12603442 Most Cited · 8 citations0.2/yr · PR 2.74ExpiredUS · Utility
Use of a cadmium-free silver alloy as brazing solder (III)
Inventors: Weise Wolfgang, Voelcker Alexander, Kaufmann Dieter, Malikowski Willi, Beuers JoergAssignee: DegussaFiled 1993-09-01 · Granted 1994-08-30

Cadmium-free brazing solders with working temperatures under 630° C. containing 45 to 80 wt. % silver, 5 to 13 wt. % copper, 10 to 25 wt. % gallium, 8 to 20 wt. % zinc, and 0 to 5 wt. % indium and/or tin.

DE 4,315,188 C1#38641158 Most Cited · 2 citations0.1/yr · PR 1.05ExpiredDE · Utility
Verwendung einer kadmiumfreien Silberlegierung als Hartlot

Cadmium-free brazing alloys having working temperatures below 630 DEG C are obtained using the following compositions: 45 to 80 % by weight of silver, 5 to 13 % by weight of copper, 10 to 25 % by weight of gallium, 8 to 20 % by weight of zinc and 0 to 5 % by weight of indium…

DE 4,315,189 C1#37503127 Most Cited · 2 citations0.1/yr · PR 1.10ExpiredDE · Utility
Verwendung einer kadmiumfreien Silberlegierung als Hartlot

Cadmium-free brazing materials with working temperatures even below 630 DEG C are obtained with the following compositions: 45 to 80% by weight of silver, 14 to 25% by weight of copper, 10 to 25% by weight of gallium, 1 to 7% by weight of zinc and 0 to 5% by weight of indium…

DE 4,315,190 C2#35521277 Most Cited · 2 citations0.1/yr · PR 1.30ExpiredDE · Utility
Verwendung von Silberlegierungen als kadmiumfreies Hartlot

Cadmium-free brazing solders which also have working temperatures under 630 DEG C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

EP 0,585,708 A1#35594636 Most Cited · 2 citations0.1/yr · PR 1.30PendingEP · Application
Use of silver alloys as cadmium-free brazing filler

Cadmium-free brazing materials with working temperatures even below 630 DEG C are obtained with the following compositions: 45 to 80% by weight of silver, 14 to 25% by weight of copper, 10 to 25% by weight of gallium, 1 to 7% by weight of zinc and 0 to 5% by weight of indium…

EP 0,586,928 A1#36074109 Most Cited · 2 citations0.1/yr · PR 1.21PendingEP · Application
Use of silver alloys as cadmium-free brazing material

Cadmium-free brazing alloys having working temperatures below 630 DEG C are obtained using the following compositions: 45 to 80 % by weight of silver, 5 to 13 % by weight of copper, 10 to 25 % by weight of gallium, 8 to 20 % by weight of zinc and 0 to 5 % by weight of indium…

DE 4,315,190 A1#97281260 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Verwendung von Silberlegierungen als kadmiumfreies Hartlot

Cadmium-free brazing solders which also have working temperatures under 630 DEG C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

DE 59,308,533 D1#127315084 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Verwendung von Silberlegierungen als kadmiumfreies Hartlot
Inventors: Voelcker Alexander Dr, Beuers Joerg Dr, Joensson Sigurd Dr, Kaufmann Dieter, Ptascheck GeorgAssignee: DegussaFiled 1993-08-16 · Granted 1998-06-18

Cadmium-free brazing solders which also have working temperatures under 630 DEG C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

DE 59,308,534 D1#81846578 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Verwendung einer kadmiumfreien Silberlegierung als Hartlot
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1998-06-18

Cadmium-free brazing materials with working temperatures even below 630 DEG C are obtained with the following compositions: 45 to 80% by weight of silver, 14 to 25% by weight of copper, 10 to 25% by weight of gallium, 1 to 7% by weight of zinc and 0 to 5% by weight of indium…

DE 59,308,535 D1#77648997 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Verwendung einer kadmiumfreien Silberlegierung als Hartlot
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1998-06-18

Cadmium-free brazing alloys having working temperatures below 630 DEG C are obtained using the following compositions: 45 to 80 % by weight of silver, 5 to 13 % by weight of copper, 10 to 25 % by weight of gallium, 8 to 20 % by weight of zinc and 0 to 5 % by weight of indium…

DK 0,585,707 T3#138742707 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDK · Utility
Anvendelse af sølvlegeringer som kadmiumfri hårdlodningsmaterialer
Inventors: Voelcker Alexander Dr, Beuers Joerg Dr, Joensson Sigurd Dr, Kaufmann Dieter, Ptascheck GeorgAssignee: DegussaFiled 1993-08-16 · Granted 1999-01-18

Cadmium-free brazing solders which also have working temperatures under 630 DEG C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

DK 0,585,708 T3#112910545 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDK · Utility
Anvendelse af en cadmiumfri sølvlegering som slaglod
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1999-01-25

Cadmium-free brazing materials with working temperatures even below 630 DEG C are obtained with the following compositions: 45 to 80% by weight of silver, 14 to 25% by weight of copper, 10 to 25% by weight of gallium, 1 to 7% by weight of zinc and 0 to 5% by weight of indium…

DK 0,586,928 T3#105734850 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDK · Utility
Anvendelse af sølvlegeringer som kadmiumfri hårdlodningsmaterialer
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1999-01-18

Cadmium-free brazing alloys having working temperatures below 630 DEG C are obtained using the following compositions: 45 to 80 % by weight of silver, 5 to 13 % by weight of copper, 10 to 25 % by weight of gallium, 8 to 20 % by weight of zinc and 0 to 5 % by weight of indium…

EP 0,585,707 A1#72652965 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Use of silver alloys as cadmium-free brazing material

Kadmiumfreie Hartlote mit Arbeitstemperaturen auch unterhalb 630 o C erhält man mit folgenden Zusammensetzungen: 45 bis 80 Gew. % Silber, 5 bis 25 Gew. % Kupfer, 10 bis 25 Gew. % Gallium und 0,1 bis 5 Gew.% Indium und/oder Zinn.

EP 0,585,707 B1#114511241 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Use of silver alloys as cadmium-free brazing material
Inventors: Voelcker Alexander Dr, Beuers Joerg Dr, Joensson Sigurd Dr, Kaufmann Dieter, Ptascheck GeorgAssignee: DegussaFiled 1993-08-16 · Granted 1998-05-13

Cadmium-free brazing solders which also have working temperatures under 630 DEG C. containing 45 to 80 wt. % silver, 5 to 25 wt. % copper, 10 to 25 wt. % gallium, and 0.1 to 5 wt. % indium and/or tin.

EP 0,585,708 B1#68688615 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Use of silver alloys as cadmium-free brazing filler
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1998-05-13

Cadmium-free brazing materials with working temperatures even below 630 DEG C are obtained with the following compositions: 45 to 80% by weight of silver, 14 to 25% by weight of copper, 10 to 25% by weight of gallium, 1 to 7% by weight of zinc and 0 to 5% by weight of indium…

EP 0,586,928 B1#144400617 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Use of silver alloys as cadmium-free brazing material
Inventors: Weise Wolfgang Dr, Voelcker Alexander Dr, Kaufmann Dieter, Malikowski Willi, Beuers Joerg DrAssignee: DegussaFiled 1993-08-16 · Granted 1998-05-13

Cadmium-free brazing alloys having working temperatures below 630 DEG C are obtained using the following compositions: 45 to 80 % by weight of silver, 5 to 13 % by weight of copper, 10 to 25 % by weight of gallium, 8 to 20 % by weight of zinc and 0 to 5 % by weight of indium…