Patents
WO 2013/078018 A2#492915 Most Cited · 70 citations5.4/yr · PR 7.96PendingWO · Application
Low density ethylene-based polymers with broad molecular weight distributions and low extractables

The invention provides an ethylene-based polymer comprising the following properties: a) a melt index (12) > 2.0 dg/min; b) a Mw(abs) versus 12 relationship: Mw(abs) < A + B(I2), where A = 2.40 x 10 5 g/mole, and B = -8.00 x 10 3 (g/mole)/(dg/min); and c) a G' versus…

WO 2013/059042 A1#608186 Most Cited · 63 citations4.8/yr · PR 6.58PendingWO · Application
Polymerization processes with fresh ethylene distributions for preparation of low density ethylene-based polymers

The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction…

WO 2010/042390 A1#1038037 Most Cited · 47 citations2.9/yr · PR 9.49PendingWO · Application
High pressure low density polyethylene resins with improved optical properties produced through the use of highly active chain transfer agents

Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…

US 9,228,036 B2#1154601 Most Cited · 45 citations4.5/yr · PR 2.92ActiveUS · Utility
Low density ethylene-based polymers with broad molecular weight distributions and low extractables

The invention provides an ethylene-based polymer comprising the following properties: a) a melt index (12)>2.0 dg/min; b) a Mw(abs) versus 12 relationship: Mw(abs)<A+B(I2), where A=2.40×10 5 g/mole, and B=−8.00×10 3 (g/mole)/(dg/min); and c) a G′ versus 12 relationship:…

US 2010087606 A1#1396158 Most Cited · 40 citations2.5/yr · PR 6.06PendingUS · Application
High pressure low density polyethylene resins with improved optical properties produced through use of highly active chain transfer agents

Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…

WO 2014/081458 A1#1766570 Most Cited · 35 citations2.9/yr · PR 4.77PendingWO · Application
Low density ethylene-based polymers with high melt strength

The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus 12 relationship: Mw(abs) < A x [(12) B ], where A = 5.00 x 10 2…

US 6,569,962 B1#1874188 Most Cited · 34 citations1.5/yr · PR 3.59ExpiredUS · Utility
Method for producing ethylene homopolymerizates and ethylene copolymerizates of a lower mass density
Inventors: Zschoch Werner, Mezquita Juan M, Beer Harald, Lohse Gerd, Berbee OttoAssignee: Dow Chemical CoFiled 1999-06-26 · Granted 2003-05-27

The invention pertains to a method for producing ethylene homopolymerizates and ethylene copolymerizates exhibiting a lower mass density of up to 0.930 g/cm 3 and a melt index ranging from 0.15 to 25 g/10 min (2.16 kg; 463 K). Said polymerizates exhibit an improved processing…

WO 2012/044504 A1#2048348 Most Cited · 32 citations2.3/yr · PR 4.60PendingWO · Application
Polymerization process to make low density polyethylene

A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a…

WO 2013/078224 A1#2057915 Most Cited · 32 citations2.5/yr · PR 4.17PendingWO · Application
Low density ethylene-based polymers with extracts at lower molecular weights

The invention provides an ethylene-based polymer comprising the following properties: A) a "weight fraction (w) of molecular weight greater than 106 g/mole, based on the total weight of polymer, and as determined by GPC(abs)," that meets the following relationship: w…

WO 2011/075465 A1#2254532 Most Cited · 30 citations2.0/yr · PR 5.32PendingWO · Application
Polymerization process to make low density polyethylene

A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising ethylene and optionally a chain transfer agent system (CTA system) into a first autoclave reactor zone operating at polymerization conditions to…

US 9,120,880 B2#2455689 Most Cited · 29 citations2.6/yr · PR 2.24ActiveUS · Utility
Polymerization processes with fresh ethylene distributions for preparation of low density ethylene-based polymers
Inventors: Zschoch Werner, Berbee Otto J, Hosman Cornelis JAssignee: Zschoch Werner, Berbee Otto JFiled 2012-10-10 · Granted 2015-09-01

The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction…

WO 2014/190036 A1#2894508 Most Cited · 26 citations2.2/yr · PR 3.11PendingWO · Application
Compositions containing low density ethylene-based polymers with high melt strength and films formed from the same

The invention provides a composition comprising the following: A) a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs) < A x [(I2) B ], where A =…

US 9,334,348 B2#3104661 Most Cited · 25 citations2.5/yr · PR 2.28ActiveUS · Utility
Low density ethylene-based polymers with extracts at lower molecular weights
Inventors: Berbee Otto J, Karjala Teresa P, Den Doelder Cornelis F J, Hinrichs StefanAssignee: Berbee Otto J, Karjala Teresa PFiled 2012-11-20 · Granted 2016-05-10

The invention provides an ethylene-based polymer comprising the following properties: A) a “weight fraction (w) of molecular weight greater than 106 g/mole, based on the total weight of polymer, and as determined by GPC(abs),” that meets the following relationship: w<A+B(I2),…

US 2014316094 A1#3300706 Most Cited · 24 citations2.0/yr · PR 2.42PendingUS · Application
Low density ethylene-based polymers with broad molecular weight distributions and low extractables

The invention provides an ethylene-based polymer comprising the following properties: a) a melt index (12)>2.0 dg/min; b) a Mw(abs) versus 12 relationship: Mw(abs)<A+B(I2), where A=2.40×10 5 g/mole, and B=−8.00×10 3 (g/mole)/(dg/min); and c) a G′ versus 12 relationship:…

US 2014316096 A1#3313653 Most Cited · 24 citations2.0/yr · PR 1.89PendingUS · Application
Low density ethylene-based polymers with extracts at lower molecular weights

The invention provides an ethylene-based polymer comprising the following properties: A) a “weight fraction (w) of molecular weight greater than 106 g/mole, based on the total weight of polymer, and as determined by GPC(abs),” that meets the following relationship: w<A+B(I2),…

US 2015274856 A1#3290546 Most Cited · 24 citations2.2/yr · PR 2.67PendingUS · Application
Low density ethylene-based polymers with high melt strength

The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus 12 relationship: Mw(abs)<A×[(12) B ], where A=5.00×10 2…

US 8,871,876 B2#3514540 Most Cited · 23 citations1.9/yr · PR 2.53ActiveUS · Utility
Ethylene-based interpolymers and processes to make the same
Inventors: Berbee Otto J, Gagnon Roger G, Jasek Mark, Nunez Laura, Gutermuth BryanAssignee: Berbee Otto J, Gagnon Roger GFiled 2011-09-21 · Granted 2014-10-28

Ethylene-based interpolymers, e.g., ethylene-acrylic acid copolymers, are made by a process comprising the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone to produce a first zone reaction…

US 9,394,389 B2#3529934 Most Cited · 23 citations2.3/yr · PR 2.14ActiveUS · Utility
Low density ethylene-based polymers with high melt strength

The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)<A×[(I2) B ], where A=5.00×10 2…

US 2016137822 A1#3773626 Most Cited · 22 citations2.2/yr · PR 2.14PendingUS · Application
Compositions containing low density ethylene-based polymers with high melt strength and films formed from the same

The invention provides a composition comprising the following: A) a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)<A×[(I2) B ], where A=5.00×10…

WO 2008/112373 A1#4193986 Most Cited · 20 citations1.1/yr · PR 3.74PendingWO · Application
A free radical initiator system and a high pressure, freeradical polymerization process for producing a low density polyethylene polymer
Inventors: Aerts Peter, Berbee OttoAssignee: Dow Global Technologies Inc, Aerts PeterFiled 2008-02-12

The instant invention is a free radical initiator system, and a high pressure, free radical polymerization process for producing a low density polyethylene polymer. The free radical initiator system according to instant invention includes at least one peroxide initiator, at…

US 8,415,442 B2#4660309 Most Cited · 19 citations1.5/yr · PR 2.29ActiveUS · Utility
High pressure low density polyethylene resins with improved optical properties produced through use of highly active chain transfer agents

Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…

WO 2012/044503 A1#4417132 Most Cited · 19 citations1.4/yr · PR 5.32PendingWO · Application
Ethylene-based interpolymers and processes to make the same

Ethylene-based interpolymers, e.g., ethylene-acrylic acid copolymers, are made by a process comprising the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone to produce a first zone reaction…

WO 2014/190041 A1#4677563 Most Cited · 19 citations1.6/yr · PR 2.06PendingWO · Application
Low density ethylene-based polymer compositions with high melt strength and mid-high density control

The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene- based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the…

WO 2015/100302 A1#4434250 Most Cited · 19 citations1.7/yr · PR 4.80PendingWO · Application
Ethylene-based polymers formed using asymmetrical polyenes

A composition comprising an ethylene-based polymer, the ethylene-based polymer having the following properties: a) at least one incorporated structure derived from a polyene selected from the group consisting of i) through x), as described herein; and b) a Mw(abs) versus I 2…

US 2014288257 A1#5495538 Most Cited · 17 citations1.4/yr · PR 1.64PendingUS · Application
Polymerization processes with fresh ethylene distributions for preparation of low density ethylene-based polymers

The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction…