CN 1,180,386 A#7587730 Most Cited · 13 citations0.5/yr · PR 2.49ExpiredCN · Utility
Process for melt spinning polyurethane and/or polyureaurethane
Inventors: Schauer G, Braeuer M, Bellmann CAssignee: Fischer Karl Ind GmbhFiled 1996-02-13

The present invention relates to a process for melt spinning polyurethane and/or polyureaurethane. In this case, an organic diisocyanate and a polymeric diol are mixed at a temperature of 50 to 150 ℃ and reacted to prepare a prepolymer. (b) The temperature is lowered by about 5…

CN 1,071,383 C#21551226 Most Cited · 5 citations0.2/yr · PR 1.37ExpiredCN · Utility
Process for melt spinning of polyurethane and/or polyurethane urea
Inventors: Schauer G, Braeuer M, Bellmann CAssignee: Fischer Karl Ind GmbhFiled 1996-02-13 · Granted 2001-09-19

The invention concerns a process for the melt spinning of polyurethane and/or polyurethane urea, in which: a) a prepolymer is produced which contains the product of reaction of an organic diisocyanate and a polymer diol by mixing at between 50 and 150 DEG C; b) the temperature…

CN 1,038,514 C#80297578 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
Melt formed from polyurethane and/or polyurethane urea elastomer
Inventors: Lehmann D, Brateuer M, Bellmann CAssignee: Fischer Karl Ind GmbhFiled 1993-01-30 · Granted 1998-05-27

A polyurethane and/or polyurethane-urea elastomer in the form of a melt which is (thermo)stable on processing and can be processed immediately or can be processed by re-melting after cooling and storage is proposed. The elastomer is prepared by a polyaddition or additive…