Patents
US 2017246707 A1#7825218 Most Cited · 13 citations1.4/yr · PR 1.81PendingUS · Application
Friction welding

A method for friction welding of inter alia coarse grain superalloy components, involving conditioning a shear zone of components to be welded by; a) pre-determining temperature profile for which the material of the shear zone of the components approaches viscoplasticity but…

US 2018209280 A1#7749756 Most Cited · 13 citations1.6/yr · PR 2.08PendingUS · Application
Bladed disc and method of manufacturing the same

A method ( 56 ) for fabricating an integral assembly ( 24 ) is disclosed. The method comprises providing ( 56 ) a first workpiece ( 26 ) having a first surface and a second workpiece ( 30 ) having a second surface ( 54 ), performing a first bonding process between the first…

US 2012012643 A1#9628591 Most Cited · 11 citations0.8/yr · PR 1.72PendingUS · Application
Process control method

A method is disclosed for controlling a process in which a component 4 is moved relative to another component 6 such that at least one of the components 4, 6 experiences a reduction in magnitude in at least one dimension. Such processes may include for example friction welding.…

US 2018073106 A1#11380207 Most Cited · 9 citations1.1/yr · PR 2.38PendingUS · Application
Nickel-base superalloy and use thereof

The novel nickel-base superalloy useful in an additive manufacturing process or a powder-based manufacturing process includes the following composition in wt %: Cr 8.0-8.5; Co 9.0-9.5; Mo 0.4-0.6; W 9.3-9.7; Ta 2.9-3.6; Al 4.9-5.6; Ti 0.2-1.0; Hf 0-0.05; C 0.005-0.03; B…

US 8,777,089 B2#16164077 Most Cited · 7 citations0.6/yr · PR 1.25ActiveUS · Utility
Process control method
Inventors: Beech Stephen M, Rowlson Michael D, Bray Simon E, Baxter Gavin J, Varia Amar MAssignee: Beech Stephen M, Rowlson Michael DFiled 2011-07-01 · Granted 2014-07-15

A method is disclosed for controlling a process in which a component 4 is moved relative to another component 6 such that at least one of the components 4, 6 experiences a reduction in magnitude in at least one dimension. Such processes may include for example friction welding.…

EP 3,293,276 A1#17744665 Most Cited · 6 citations0.8/yr · PR 1.62PendingEP · Application
Nickel-base superalloy and use thereof
Inventors: Hardy Mark, Gibson Grant, Baxter Gavin, Pardhi YogirajAssignee: Rolls Royce PlcFiled 2017-09-05

The novel nickel-base superalloy useful in an additive manufacturing process or a powder-based manufacturing process comprises the following composition in wt%: the balance nickel and incidental elements and unavoidable impurities.

US 10,752,978 B2#18917730 Most Cited · 6 citations1.0/yr · PR 1.16ActiveUS · Utility
Nickel-base superalloy and use thereof
Inventors: Hardy Mark C, Gibson Grant J, Baxter Gavin J, Pardhi YogirajAssignee: Rolls Royce PlcFiled 2017-09-06 · Granted 2020-08-25

The novel nickel-base superalloy useful in an additive manufacturing process or a powder-based manufacturing process includes the following composition in wt %: Cr 8.0-8.5; Co 9.0-9.5; Mo 0.4-0.6; W 9.3-9.7; Ta 2.9-3.6; Al 4.9-5.6; Ti 0.2-1.0; Hf 0-0.05; C 0.005-0.03; B…

US 2012012644 A1#26908514 Most Cited · 4 citations0.3/yr · PR 1.14PendingUS · Application
Apparatus and a method of determining the quality of a friction weld

A method of determining the quality of a friction weld between two components, the method comprising joining two components together using a friction welding process, measuring the loss of length of the components as a function of time during the friction welding process,…

EP 2,975,737 A2#45572057 Most Cited · 2 citations0.2/yr · PR 0.85PendingEP · Application
Negative pressure motor sealing
Inventors: Shuck Quinlan Yee, Baxter GavinAssignee: Rolls Royce Corp, Rolls Royce PlcFiled 2015-07-14

A system includes an electric motor including a housing enclosing a substantially-sealed internal environment, a pump including an inlet connected to the substantially-sealed internal environment of the electric motor via a first conduit, and a fluid supply storing a makeup…

EP 3,095,551 A1#34533538 Most Cited · 2 citations0.2/yr · PR 1.75PendingEP · Application
Additive layer repair of a metallic component
Inventors: Heason Christopher, Baxter GavinAssignee: Rolls Royce PlcFiled 2016-05-13

A method of repairing a metallic component (100) (formed from a first material (110)) by powder feeding laser deposition, comprises the step of depositing a plurality of first repair layers (130) onto a repair surface (120) of the component (100) to form a first repair zone…

EP 3,213,856 A1#45552371 Most Cited · 2 citations0.2/yr · PR 0.85PendingEP · Application
Process for conditioning of a shear zone for friction welding
Inventors: Bray Simon, Walpole Andrew, Forsdike John, Baxter GavinAssignee: Rolls Royce PlcFiled 2017-01-31

A method suitable for the friction welding of inter alia coarse grain superalloy components is described. The method involves conditioning a shear zone of components to be welded by; a) pre-determining a temperature profile for which the material of the shear zone of the…

US 2016341044 A1#43723903 Most Cited · 2 citations0.2/yr · PR 0.92PendingUS · Application
Additive layer repair of a metallic component
Inventors: Heason Christopher P, Baxter Gavin JAssignee: Rolls Royce PlcFiled 2016-05-13

A method of repairing a metallic component (formed from a first material) by powder feeding laser deposition, comprises the step of depositing a plurality of first repair layers onto a repair surface of the component to form a first repair zone, the first of the plurality of…

US 2024068074 A1#40856724 Most Cited · 2 citations1.0/yr · PR 0.99PendingUS · Application
Titanium alloy and methods of manufacture
Inventors: Lister Samuel T, Baxter Gavin J, Jackson MartinAssignee: Rolls Royce PlcFiled 2023-08-18

A titanium alloy comprising Al 4.78 to 6.44 wt. %; V 3.65 to 5.15 wt. %; Mo 1.32 to 3.58 wt. %; Cr 0.75 to 2.28 wt. %; Fe 0.00 to 0.42 wt. %; C 0.00 wt. % to 0.10 wt. %; S 0.00 wt. % to 0.10 wt. %; N up to 500 ppm; O up to 2000 ppm and H up to 150 ppm; the balance being Ti and…

US 8,342,382 B2#44367595 Most Cited · 2 citations0.1/yr · PR 0.91ActiveUS · Utility
Determining the quality of a friction weld using a double differential
Inventors: Baxter Gavin J, Horwell Mark G, Bray Simon EAssignee: Rolls Royce Plc, Baxter Gavin JFiled 2011-02-04 · Granted 2013-01-01

A method of determining the quality of a friction weld between two components, the method comprising joining two components together using a friction welding process, measuring the loss of length of the components as a function of time during the friction welding process,…

EP 2,407,270 A2#48780968 Most Cited · 1 citations0.1/yr · PR 0.89PendingEP · Application
Process control method for inertial friction welding

A method is disclosed for controlling a process in which a component 4 is moved relative to another component 6 such that at least one of the components 4, 6 experiences a reduction in magnitude in at least one dimension. Such processes may include for example friction welding.…

EP 2,361,715 A1#96578965 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
An apparatus and a method of determining the quality of a friction weld
Inventors: Baxter Gavin, Horwell Mark, Bray SimonAssignee: Rolls Royce PlcFiled 2011-02-04

A method of determining the quality of a friction weld between two components, the method comprising joining two components together using a friction welding process, measuring the loss of length of the components as a function of time during the friction welding process,…

EP 2,407,270 A3#75388288 Most Cited · 0 citations0.0/yr · PR 0.56ActiveEP · Utility
Process control method for inertial friction welding

A method is disclosed for controlling a process in which a component 4 is moved relative to another component 6 such that at least one of the components 4, 6 experiences a reduction in magnitude in at least one dimension. Such processes may include for example friction welding.…

EP 2,975,737 A3#119781582 Most Cited · 0 citations0.0/yr · PR 0.56ActiveEP · Utility
Negative pressure motor sealing
Inventors: Shuck Quinlan Yee, Baxter GavinAssignee: Rolls Royce Corp, Rolls Royce PlcFiled 2015-07-14

A system includes an electric motor including a housing enclosing a substantially-sealed internal environment, a pump including an inlet connected to the substantially-sealed internal environment of the electric motor via a first conduit, and a fluid supply storing a makeup…

EP 3,760,363 A1#135502240 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method of joining by welding a first component to a second component with a local surface treatment before joining

The present application relates to a method of joining a first component to a second component at respective connection surfaces, comprising, in order, applying a local surface treatment (step 100) to the connection surface of at least one of the first and second components in…

EP 4,327,964 A1#99488596 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Titanium alloy and methods of manufacture
Inventors: Lister Samuel T, Baxter Gavin J, Jackson MartinAssignee: Rolls Royce PlcFiled 2023-07-25

A titanium alloy comprising Al 4.78 to 6.44 wt.%; V 3.65 to 5.15 wt.%; Mo 1.32 to 3.58 wt.%; Cr 0.75 to 2.28 wt.%; Fe 0.00 to 0.42 wt.%; C 0.00 wt.% to 0.10 wt.%; S 0.00 wt.% to 0.10 wt.%; N up to 500 ppm; O up to 2000 ppm and H up to 150 ppm; the balance being Ti and incidental…

GB 2,482,003 A#79642938 Most Cited · 0 citations0.0/yr · PR 0.56ActiveGB · Utility
Method of controlling a process such as friction welding

A method is disclosed for controlling a process in which a component 4 is moved relative to another component 6 such that at least one of the components 4, 6 experiences a reduction in magnitude in at least one dimension. Such processes may include for example friction / inertia…