Process for the preparation of sulphate pulp from a lignocellulose-containing material. The yield of the pulp can be raised here because of the very short time of contact between the material and the cooking liquor in the temperature range of 80-140 degrees C. The impregnation…
Methods of manufacturing sulphate pulp from lignocellulose-contain-ing material are disclosed. The yields obtainable in such methods are increased by assuring that the time during which the lignocellulose-containing material is in contact with the cooking liquor at a temperature…
The coarser reject panes from the sieve via a conveyor to an impregnation stage where it is treated with excess lye preferably at atmospheric pressure at temp. 80 deg.C for 10 hrs. Pref. the ratio of wood to lye is 1:6. Then the lye is run off. The treated chips and the…