Foldable substrates have a first portion, a second portion, and a central portion positioned therebetween with a first transition region having a first central surface area of the central portion with a first average angle. In aspects, the first average angle is from about…
Aize Li
Apparatus and method for treating a substrate, for example texturing a substrate. In some embodiments, a masking material is applied to a surface of the substrate in a predetermined pattern, the surface thereafter contacted with an etchant that removes the masking material.…
A textured glass article includes: a body comprising an aluminosilicate glass comprising greater than or equal to 16 wt % Al 2 O 3 and a Al 2 O 3 /SiO 2 ratio less than or equal to 0.3, the body having at least a first surface; a plurality of polyhedral surface features…
A borosilicate-based composition, including: 50-85 mol. % SiO 2 , 10-40 mol. % B 2 O 3 , > 0-5 mol. % SnO 2 , and > 0-20 mol. % of at least one alkali oxide selected from Li 2 O, Na 2 O, K 2 O, Rb 2 O, and Cs 2 O, such that the composition has a Young's Modulus less than 64 GPa.
The methods generally include contacting an alkali-containing glass article having a first alkali metal cation with a molten salt bath including from 0.1 wt. % to 3 wt. % nanoparticles and at least one alkali metal salt having a second alkali metal cation that has an atomic…
A glass article is provided that includes: a glass substrate comprising a thickness and a primary surface; and a textured region defined by the primary surface. The textured region comprises a low spatial frequency region and a high spatial frequency region substantially…
Described herein are textured glass-based articles. The textured glass based articles may include a glass-based substrate including a first major surface and a second major surface. At least a portion of one or both of the first major surface and the second major surface is…
A silicate-based glass composition includes 15-65 wt. % SiO 2 , 15-50 wt. % CaO, 1-30 wt. % P 2 O 5 , and 1-20 wt. % ZrO 2 , such that the composition has a hydrolytic resistance of glass grains (HGB) of at most 3, when measured by International Organization for Standardization…
The present disclosure relates to a quantum dot-doped glass and method of making the same. A quantum dot-doped glass includes glass that includes quantum dots in an internal structure of the glass. The quantum dots within the glass have a photoluminescence quantum yield of…
A silicate-based glass composition includes 15-65 wt. % SiO 2 , 2.5-25 wt. % MgO, 1-30 wt. % P 2 O 5 , and 15-50 wt. % CaO, such that the composition has a hydrolytic resistance of glass grains (HGB) of at most 3, when measured by International Organization for Standardization…
An aqueous dentifrice formulation, comprising: a bioactive glass exhibiting at least one of: a hydrolytic resistance of glass grains (HGB) of at most 4, when measured by International Organization for Standardization section 719 (ISO 719); a weight loss of 5 wt. % or less after…
A coated textured glass article is described herein that comprises: a glass body comprising a first surface; a plurality of polyhedral surface features extending from the first surface; and a coating disposed on the first surface of the body and the plurality of polyhedral…
A method of making a glass article using a phase separated silicate glass including a silica rich first phase and a boron rich second phase. The phase separated silica glass is etched with an etchant to remove at least a portion of the second phase and obtain a high silica…
A method of forming a glass laminate includes providing a substrate having a core layer and at least one cladding layer; heat treating the substrate at a temperature such that the at least one cladding layer is phase-separated after the heat treating; and etch treating the…
The methods generally include contacting an alkali-containing glass article having a first alkali metal cation with a molten salt bath including from 0.1 wt. % to 3 wt. % nanoparticles and at least one alkali metal salt having a second alkali metal cation that has an atomic…
A glass article is provided that includes: a glass substrate comprising a thickness and a primary surface; and a textured region defined by the primary surface. The textured region comprises a low spatial frequency region and a high spatial frequency region substantially…
Described herein are textured glass-based articles. The textured glass-based articles may include a glass-based substrate including a first major surface and a second major surface. At least a portion of one or both of the first major surface and the second major surface is…
Methods of treating a glass substrate including heating the glass substrate at a first temperature for a first period of time from greater than or equal to 1 minute to less than or equal to 2 hours to form a heat-treated glass substrate. The first temperature is less than an…
A silicate-based glass composition includes 15-65 wt. % SiO 2 , 15-50 wt. % CaO, 1-30 wt. % P 2 O 5 , and 1-20 wt. % ZrO 2 , such that the composition has a hydrolytic resistance of glass grains (HGB) of at most 3, when measured by International Organization for Standardization…
A silicate-based glass composition includes 15-65 wt. % SiO 2 , 2.5-25 wt. % MgO, 1-30 wt. % P 2 O 5 , and 15-50 wt. % CaO. The glass composition may also include 0-5 wt. % F − , and 0-10 wt. % ZrO 2 . The glass composition may also include one of 0-10 wt. % Al 2 O 3 , 0-10 wt.…
Glass-based substrates have a substrate thickness from 20 micrometers to 200 micrometers and a depletion layer extending from a first major surface to a first depth from 1 nanometers to 75 nanometers. The depletion layer is depleted in one or more alkali metal oxide, alkaline…
The present disclosure relates to a quantum dot-doped glass and method of making the same. A quantum dot-doped glass includes glass that includes quantum dots in an internal structure of the glass. The quantum dots within the glass have a photoluminescence quantum yield of…