US 2005275096 A1#536484 Most Cited · 67 citations3.2/yr · PR 8.28PendingUS · Application
Pre-doped reflow interconnections for copper pads
Inventors: Zeng Kejun, Chiu Tz-cheng, Holdford Rebecca LAssignee: Zeng Kejun, Chiu Tz-chengFiled 2004-08-16

A metal interconnect structure ( 100 ) comprising a bond pad ( 110 ) of copper; a body ( 103 ) of eutectic alloy in contact with the bond pad, this alloy including copper; and a contact pad ( 120 ) comprising copper in contact with the alloy body. When the eutectic alloy is…

US 2012001336 A1#1294495 Most Cited · 42 citations3.0/yr · PR 4.75PendingUS · Application
Corrosion-resistant copper-to-aluminum bonds
Inventors: Zeng Kejun, Peng Wei QunAssignee: Zeng Kejun, Peng Wei QunFiled 2010-07-02

A connection formed by a copper wire ( 112 ) alloyed with a noble metal in a first concentration bonded to a terminal pad ( 101 ) of a semiconductor chip; the end of the wire being covered with a zone ( 302 ) including an alloy of copper and the noble metal in a second…

US 2006267157 A1#4596966 Most Cited · 19 citations0.9/yr · PR 2.88PendingUS · Application
Solder joints for copper metallization having reduced interfacial voids

A metal interconnect structure ( 100 ) comprising a bond pad ( 101 ), which has copper with at least 70 volume percent composed of crystal grains expanding more than 1 μm in their main direction, and 30 or less volume percent composed of crystal grains, which expand less than 1…

WO 2008/154471 A2#17323588 Most Cited · 6 citations0.3/yr · PR 1.76PendingWO · Application
Stable gold bump solder connections

A metallic interconnect structure (200) for connecting a gold bump (205) and a copper pad (212), as used for example in semiconductor flip-chip assembly. A first region (207) of binary AuSn2 intermetallic is adjacent to the gold bump. A region (208) of binary AuSn4 intermetallic…

US 2006038302 A1#19475488 Most Cited · 5 citations0.2/yr · PR 2.05PendingUS · Application
Thermal fatigue resistant tin-lead-silver solder
Inventors: Zeng KejunAssignee: Zeng KejunFiled 2004-08-19

A solder comprising a ternary alloy of tin, lead, and silver, providing approximately the eutectic melting temperature and about 0.7 to 1.5 weight percent silver. In one embodiment, the ternary solder alloy comprises the composition of about 61.0 weight percent tin, about 37.5…

US 2006097398 A1#19010087 Most Cited · 5 citations0.2/yr · PR 4.33PendingUS · Application
Method and structure to reduce risk of gold embrittlement in solder joints
Inventors: Zeng KejunAssignee: Zeng KejunFiled 2005-12-13

A method for reducing gold embrittlement in solder joints, and a copper-bearing solder according to the method, are disclosed. Embodiments of the invention comprise adding copper to non-copper based solder, such as tin-lead solder. The embodiments may further comprise using the…

CN 207,637,385 U#58405904 Most Cited · 1 citations0.1/yr · PR 0.78ActiveCN · Utility
The full parabola light propagation demonstration device of adjustable water flow
Inventors: Zeng KejunAssignee: Zeng KejunFiled 2017-09-21 · Granted 2018-07-20

The utility model is the full parabola light propagation demonstration device of adjustable water flow, solve have light propagation demonstration device tank and water jet one, the firing angle of flow and hydraulic pressure are non-adjustable, inconvenience is observed when…

WO 2008/043010 A2#49149187 Most Cited · 1 citations0.1/yr · PR 0.89PendingWO · Application
Gold-tin solder joints having reduced embrittlement

A metal interconnection for two workpieces such as a semiconductor chip and an insulating substrate. The first workpiece (101) has a first contact pad (201) with a gold stud (110); the second workpiece (103) is covered with an insulating layer (213) and a window in the layer to…

CN 107,424,495 A#136132220 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
The full parabola light propagation demonstration device of adjustable water flow
Inventors: Zeng KejunAssignee: Zeng KejunFiled 2017-09-21

The present invention is the full parabola light propagation demonstration device of adjustable water flow, solve existing light propagation demonstration device tank and water jet one, the firing angle of current and hydraulic pressure are non-adjustable, inconvenience…

WO 2005/087430 A1#96797553 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method of semi-conductor device assembly including fatigue-resistant ternary solder alloy
Inventors: Zeng KejunAssignee: Texas Instruments Inc, Zeng KejunFiled 2005-03-09

Method for assembling a semiconductor device having fatigue-resistant interconnection fillet provides a semiconductor chip with at least one solder bump comprising an alloy of tin and lead with a melting temperature higher than the solder paste used. Further, a solder paste…

WO 2006/023914 A2#117257093 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Thermal fatigue resistant tin-lead-silver solder
Inventors: Zeng KejunAssignee: Texas Instruments Inc, Zeng KejunFiled 2005-08-19

A solder comprising a ternary alloy of tin, lead, and silver, providing approximately the eutectic melting temperature and about 0.7 to 1.5 weight percent silver. In one embodiment, the ternary solder alloy comprises the composition of about 61.0 weight percent tin, about 37.5…

WO 2006/023914 A3#81468045 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Thermal fatigue resistant tin-lead-silver solder
Inventors: Zeng KejunAssignee: Texas Instruments Inc, Zeng KejunFiled 2005-08-19

A solder comprising a ternary alloy of tin, lead, and silver, providing approximately the eutectic melting temperature and about 0.7 to 1.5 weight percent silver. In one embodiment, the ternary solder alloy comprises the composition of about 61.0 weight percent tin, about 37.5…

WO 2006/130609 A1#120104014 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Solder joints for copper metallization having reduced interfacial voids

A metal interconnect structure (100) comprising a bond pad (101), which has copper with at least 70 volume percent composed of crystal grains expanding more than 1 μm in their main direction, and 30 or less volume percent composed of crystal grains, which expand less than 1 μm…

WO 2008/043010 A3#93179673 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Gold-tin solder joints having reduced embrittlement

A metal interconnection for two workpieces such as a semiconductor chip and an insulating substrate. The first workpiece (101) has a first contact pad (201) with a gold stud (110); the second workpiece (103) is covered with an insulating layer (213) and a window in the layer to…

WO 2008/154471 A3#108957094 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Stable gold bump solder connections

A metallic interconnect structure (200) for connecting a gold bump (205) and a copper pad (212), as used for example in semiconductor flip-chip assembly. A first region (207) of binary AuSn2 intermetallic is adjacent to the gold bump. A region (208) of binary AuSn4 intermetallic…

WO 2009/140238 A2#153516454 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Structure and method for reliable solder joints

A solder joint (200) has a first contact pad (114) and a second contact pad (124) of a first metal, preferably copper, facing each other across a gap. A coat (115 and 125, respectively) of a second metal, preferably nickel, covers each pad. A layer (201) of crystals of first…

WO 2009/140238 A3#138986798 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Structure and method for reliable solder joints

A solder joint (200) has a first contact pad (114) and a second contact pad (124) of a first metal, preferably copper, facing each other across a gap. A coat (115 and 125, respectively) of a second metal, preferably nickel, covers each pad. A layer (201) of crystals of first…

WO 2012/003315 A2#118300001 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Corrosion-resistant copper-to-aluminum bonds

A connection is formed by a copper wire (112) alloyed with a noble metal in a first concentration bonded to a terminal pad (101) of a semiconductor chip. The end of the wire is covered with a zone including an alloy of copper and the noble metal in a second concentration higher…

WO 2012/003315 A3#85996756 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Corrosion-resistant copper-to-aluminum bonds

A connection is formed by a copper wire (112) alloyed with a noble metal in a first concentration bonded to a terminal pad (101) of a semiconductor chip. The end of the wire is covered with a zone including an alloy of copper and the noble metal in a second concentration higher…