A 7000 aluminum alloy extrudate that suppresses natural aging of proof strength value, etc. through inhibiting of positive effects by unattended leaving at ordinary temperature after extrusion forming and excels in impact resistance performance. For the suppression of natural…
Yoshida Tomoo
The purpose of the present invention is to provide a high-strength aluminum alloy with excellent extrudability and resistance to stress corrosion cracking, and a method of manufacturing extrusions using said aluminum alloy. The aluminum alloy which solves achieves this purpose…
An aluminum alloy extruded product includes an aluminum alloy including 6.0 to 7.2 mass % of Zn, 1.0 to 1.6 mass % of Mg, 0.1 to 0.4 mass % of Cu, at least one component selected from the group consisting of Mn, Cr, and Zr in a respective amount of 0.25 mass % or less and a…
An aluminum alloy extruded product includes an aluminum alloy including 6.0 to 7.2 mass % of Zn, 1.0 to 1.6 mass % of Mg, 0.1 to 0.4 mass % of Cu, at least one component selected from the group consisting of Mn, Cr, and Zr in a respective amount of 0.25 mass % or less and a…
A high-strength aluminum alloy exhibiting excellent stress corrosion cracking resistance and excellent extrudability, and a method for producing an extruded shape using the same are disclosed. The aluminum alloy includes 1.6 to 2.6 mass % of Mg, 6.0 to 7.0 mass % of Zn, 0.5 mass…
A bactericide for MRSA, characterized in that it comprises a product prepared by pulverizing a shell having a crystalline structure of a calcite type of calcium carbonate. The bactericide allows a wide variety of articles to be sterilized by the use of one type of bactericide,…
A 6000 aluminum extrudate containing, by mass, 0.3-0.7% magnesium, 0.7-1.5% silicon, 0.35% or less copper, 0.35% or less iron and 0.005-0.1% titanium, and further containing 0.05-0.30% manganese, 0.10% or less chromium and 0.10% or less zirconium provided that at least one…
A high-strength aluminum alloy exhibiting excellent stress corrosion cracking resistance and excellent extrudability, and a method for producing an extruded shape using the same are disclosed. The aluminum alloy includes 1.6 to 2.6 mass % of Mg, 6.0 to 7.0 mass % of Zn, 0.5 mass…
This invention relates to a 6000-series aluminum extruded material containing magnesium (0.3% to 0.7% by mass), silicon (0.7% to 1.5% by mass), copper (0.35% or less by mass), iron (0.35% or less by mass), titanium (0.005% to 0.1% by mass), manganese (0.05% to 0.30% by mass),…
A method includes: preparing a molten aluminum alloy consisting of 0.3-0.8 mass % Mg, 0.5-1.2 mass % Si, 0.3 mass % or more excess Si relative to the Mg 2 Si stoichiometric composition, 0.05-0.4 mass % Cu, 0.2-0.4 mass % Mn, 0.1-0.3 mass % Cr, 0.2 mass % or less Fe, 0.2 mass %…