The present invention relates to a product of ferritic stainless steel manufactured according to the process of this invention, which product has increased resistance to cyclic and continuous thermal load and oxidation at elevated temperatures and which has improved mechanical…
Witt Eva
Ferritic steel alloyed with a balanced quantity of chromium, aluminium and reactive elements and that has the following composition (in % by weight): Ni up to 1 Cr 15-25 Al 0.75-3.7 Si max 0.6 Mo and/or W 0-3 Ti and/or Nb 0-1 Cup to 0.2 N up to 0.2 one or more of the reactive…
The present invention relates to a product of ferritic stainless steel manufactured according to the process of this invention, which product has increased resistance to cyclic and continuous thermal load and oxidation at elevated temperatures and which has improved mechanical…
The present invention relates to a method to produce an austenitic alloy by an austenitic stainless substrate alloy of low Al content being coated with an alloy of higher Al content at a temperature between 100° C. and 600° C., so that the resulting product has an Al content of…
Ferritic steel alloyed with a balanced quantity of chromium, aluminium and reactive elements and that has the following composition (in % by weight): Ni up to 1 Cr 15-25 Al 0,75-3,7 Si max 0,6 Mo and/or W 0-3 Ti and/or Nb 0-1 Cup to 0,2 N up to 0,2 one or more of the reactive…
The present invention relates to a method to produce an austenitic alloy by an austenitic stainless substrate alloy of low Al content being coated with an alloy of higher Al content at a temperature between 100 °C and 600 °C, so that the resulting product has an Al content of…
Ferritic steel alloyed with a balanced quantity of chromium, aluminium and reactive elements and that has the following composition (in % by weight): Ni up to 1 Cr 15-25 Al 0,75-3,7 Si max 0,6 Mo and/or W 0-3 Ti and/or Nb 0-1 Cup to 0,2 N up to 0,2 one or more of the reactive…