A high-temperature component made of a nickel super-alloy has the following composition in wt %: 11-13% of Cr, 3-5% of W, 0.5-2.5% of Mo, 3-5% of Al, 3-5% of Ti, 3-7% of Ta, 1-5% of Re and a remainder formed of nickel. A corresponding component which is also provided is formed…
Winfried Esser
A metallic layer is cooled below room temperature, leading to an embrittlement. Subsequently, the metallic layer is stripped by performing a blasting process having a high efficiency because of the brittleness. Additionally, the substrate is prevented from being damaged by using…
During a solution heat treatment grain recrystallization may occur of a textured article, especially at the surface rim. The present invention provides a method for restoring the microstructure of a textured article, which comprises coating the surface of the article with a high…
In a method of producing a turbine blade in hollow section, an especially low defect or scrap rate is to be ensured. To this end, a first core element is connected via a number of approximately cylindrical spacers to a further core element and/or to a casting mold, the cavities…
During a solution heat treatment grain recrystallization may occur of a textured article, especially at the surface rim. The present invention provides a method for restoring the microstructure of a textured article, such as a gas turbine engine blade, which comprises coating…