The invention provides a method for preparing particulate brucite comprising grinding and beneficiating particulate brucite wherein the ground beneficiated particulate brucite has a d90 of less than or equal to about 6.4μm as measured by laser light scattering.
Assignee / Organization
Windebank Mark Barry
0Total Forward Citations
1Indexed Patents
0Avg Citations / Patent
0Portfolio H-Index