Patents
Assignee / Organization

Weisweiler Werner

36Total Forward Citations
10Indexed Patents
4Avg Citations / Patent
4Portfolio H-Index
DE 19,756,392 A1#9988074 Most Cited · 10 citations0.4/yr · PR 2.90PendingDE · Application
Removal of nitrogen oxides from waste gas using an iron oxyhydroxide catalyst
Inventors: Weisweiler Werner Prof DrAssignee: Weisweiler Werner Prof DrFiled 1997-12-18

NOx is removed from oxygen-containing waste gas using a catalyst made of iron oxyhydroxide containing combined water. NOx removal from oxygen-containing waste gases is effected by contacting the gases at 200-500 deg C in the presence of ammonia or an ammonia source in a NOx:NH3…

DE 4,140,969 A1#14645490 Most Cited · 7 citations0.2/yr · PR 2.15PendingDE · Application
Mercury (cpd.) sepn. from gas - by amalgamation, evapn. with flushing gas and condensation
Inventors: Weisweiler Werner Prof DrAssignee: Weisweiler Werner Prof DrFiled 1991-12-12

In mercury (cpd.) sepn. and recovery from gases (esp. waste gases from thermal processes) by amalgamation with a supported metal, the novelty is that (a) the gases are passed at a space velocity of 1000-10,000/hr. at 20-250 deg.C under reducing conditions, over a supported…

WO 9,967,512 A1#19734763 Most Cited · 5 citations0.2/yr · PR 1.85PendingWO · Application
Exhaust emission control system for denoxing exhaust gases from combustion units and method therefor

An exhaust emission control system for denoxing exhaust gases from combustion units on a SCR converter comprising a heateable, pressure-resistant converter containing a substace or a corresponding mixture of substances that thermolytically separate(s) NH3, an NH3 store for…

WO 9,851,402 A1#23444385 Most Cited · 4 citations0.1/yr · PR 1.68PendingWO · Application
Method and device for reducing nitrogen oxides in an scr catalyst

The invention relates to a method for reducing nitrogen oxides in an SCR catalyst, which is arranged in the exhaust gas line of an internal combustion engine, with ammonia (NH3) which is introduced in front of the catalyst in the exhaust gas flow and comprising the following…

DE 19,520,548 A1#28639274 Most Cited · 3 citations0.1/yr · PR 1.46PendingDE · Application
Recovery of energetic components from plastic-bonded propellants etc.

A process for the recovery of energetic components (I) from plastic-bonded propellants and explosives (II) comprises decomposition at 0-500 (pref. 2-50) bar and 80-250 (pref. 100-190) deg C for 5 mins. to 5 hrs. with an aq. solvolytic agent contg. various additives.

EP 0,981,403 A1#116424369 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method and device for reducing nitrogen oxides in an scr catalyst

The invention relates to a method for reducing nitrogen oxides in an SCR catalyst, which is arranged in the exhaust gas line of an internal combustion engine, with ammonia (NH3) which is introduced in front of the catalyst in the exhaust gas flow and comprising the following…

WO 9,851,402 A8#64547406 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Method and device for reducing nitrogen oxides in an scr catalyst

The invention relates to a method for reducing nitrogen oxides in an SCR catalyst, which is arranged in the exhaust gas line of an internal combustion engine, with ammonia (NH3) which is introduced in front of the catalyst in the exhaust gas flow and comprising the following…