A flux for hot dip galvanization comprises from:• 60 to 80 wt.% of zinc chloride (ZnCl2); 7 to 20 wt.% of ammonium chloride (NH4Cl); 2 to 20 wt.% of a fluidity modifying agent comprising at least one alkali or alkaline earth metal; 0.1 to 5 wt.% of a least one of the following…
Warichet David
The present invention generally relates to a flux for hot dip galvanization comprising from: 36 to 80 wt. % (percent by weight) of zinc chloride (ZnC12); 8 to 62 wt.% of ammonium chloride (NH4C); from 2,0 to 10 wt. % of a least one of the following compounds: NiC12, MnC12 or a…
The present invention generally relates to a flux for hot dip galvanization comprising from: 36 to 80 wt. % (percent by weight) of zinc chloride (ZnCl2); 8 to 62 wt. % of ammonium chloride (NH4C); from 2.0 to 10 wt. % of a least one of the following compounds: NiCl2, MnCl2 or a…
The invention concerns a method for treating waste stripping solutions to obtain ferrous chloride solutions sufficiently concentrated in whole iron and depleted in zinc and other metal impurities. The method comprises three successive operational steps: a first step for…
The present invention generally relates to a flux for hot dip galvanization comprising from: 36 to 80 wt. % (percent by weight) of zinc chloride (ZnCl2); 8 to 62 wt. % of ammonium chloride (NH4C); from 2.0 to 10 wt. % of a least one of the following compounds: NiCl2, MnCl2 or a…