An insertion device (100, 1100) for inserting an infusion device (102) at least partially into skin for subcutaneous infusion can comprise a sleeve (106, 1106) having a lower surface (176) that is configured to engage the skin, a shuttle or carriage (116, 1116) to carry the…
Walker Joseph K
A low VOC, HAPs free, substantially non-aqueous slurry for use as a rheology modifier in aqueous systems including but not limited to latex paints. The slurry comprises a particulate water-swelling polymer such as hydroxyethyl cellulose, mineral oil carrier liquid, a non-ionic…
An insertion device for inserting an infusion device at least partially into skin for subcutaneous infusion can comprise a sleeve having a lower surface that is configured to engage the skin, a shuttle or carriage to carry the infusion device between a retracted position and an…
The present invention is directed to smoke suppressants based on ammonium octamolybdate chemistry. According to this invention, the precipitation of ammonium octamolybdate in the presence of an inert mineral core produce a novel high surface area ammonium octamolybdate smoke…
The smoke suppressant comprises a molybdate precipitate on the surface of a borate core. The precipitate increases surface area of the core and provides improved smoke suppression relative to a mixture of the molybdate and borate core. The suppressants can be incorporated into…
The present invention is directed to smoke suppressants based on ammonium octamolybdate chemistry. According to this invention, the precipitation of ammonium octamolybdate in the presence of an inert mineral core produce a novel high surface area ammonium octamolybdate smoke…
A coating composition comprising: (i) at least one polyepoxide; (ii) at least one polyvinyl butyral resin; (iii)a corrosion inhibiting amount of cerium phosphate; (v) phosphoric acid; (v) a water miscible organic solvent; and (vii) water; wherein the coating composition is free…
The smoke suppressant comprises a molybdate precipitate on the surface of a borate core. The precipitate increases surface area of the core and provides improved smoke suppression relative to a mixture of the molybdate and borate core. The suppressants can be incorporated into…
A low VOC, HAPs free, substantially non-aqueous slurry for use as a rheology modifier in aqueous systems including but not limited to latex paints is disclosed. The slurry comprises a particulate water-swelling polymer such as hydroxyethyl cellulose, mineral oil carrier liquid,…
The present invention is directed to smoke suppressants based on ammonium octamolybdate chemistry. According to this invention, the precipitation of ammonium octamolybdate in the presence of an inert mineral core produce a novel high surface area ammonium octamolybdate smoke…
A coating composition comprising: (i) at least one polyepoxide; (ii) at least one polyvinyl butyral resin; (iii)a corrosion inhibiting amount of cerium molybdate; (v) phosphoric acid; (v) a water miscible organic solvent; and (vii) water; wherein the coating composition is free…
A coating composition comprising: (i) at least one polyepoxide; (ii) at least one polyvinyl butyral resin; (iii)a corrosion inhibiting amount of cerium phosphate; (v) phosphoric acid; (v) a water miscible organic solvent; and (vii) water; wherein the coating composition is free…
The smoke suppressant comprises a molybdate precipitate on the surface of a borate core. The precipitate increases surface area of the core and provides improved smoke suppression relative to a mixture of the molybdate and borate core. The suppressants can be incorporated into…