A process for producing silicon wafers with low defect density is one wherein a) a silicon single crystal having an oxygen doping concentration of at least 4*10 17 /cm 3 is produced by molten material being solidified to form a single crystal and is then cooled, and the holding…
wacker-siltronic
A method for cutting up a workpiece which is in rod or block form by means of a saw, wherein the temperature of the workpiece is measured during the cutting, and the measurement signal is transmitted to a control unit, which generates a control signal which is used to control…
A wire saw for, and a method of, cutting off slices from a workpiece. The re saw has a cutting head, which contains a plurality of wire guide rollers and around which a multiplicity of wire sections lying parallel to one another and forming plane wire webs are moved, a holding…
A process for the surface polishing of a silicon wafer, includes the successive polishing of the silicon wafer on at least two different polishing plates covered with polishing cloth, with a continuous supply of alkaline polishing abrasive with SiO 2 constituents, an amount of…
There is a process for producing a semiconductor wafer having a front surface and a back surface and a polished edge, in which the semiconductor wafer is subjected to polishing on both sides. The process includes the following temporal sequence of steps: (a) polishing of the…
A process is for material-removing machining, on both sides simultaneously, of semiconductor wafers having a front surface and a back surface, the semiconductor wafers resting in carriers which are set in rotation by means of an annular outer drive ring and an annular inner…
Apparatus for producing a single crystal of semiconductor material in accance with the Czochralski method, has a cooling means which cools the growing single crystal and is constructed in two parts, The first is an upper part duct system through which a liquid coolant flows. The…
A method for cutting a multiplicity of disks from a hard brittle workpiece is by moving the workpiece at a defined feed rate through a wire web of a wire saw. In the method, the wire web is formed by a sawing wire which moves in a reciprocating manner and is covered with bonded…
A sawing method and a wire saw for cutting wafers from a workpiece comprises a guidance system for the guidance of wire segments into the intended cutting planes, having at least one measuring device and at least one controlling device, the measuring device detecting an…
A process for producing a silicon single crystal has the crystal being pulled using the Czochralski method while being doped with oxygen and nitrogen. The single crystal is doped with oxygen at a concentration of less than 6.5*10 17 atoms cm −3 and with nitrogen at a…
PROBLEM TO BE SOLVED: To provide a manufacturing method, in which a silicon wafer, which has low defect density in an area especially near a surface and whose oxygen doping concentration is at least 4×10<17> /cm<3> , is obtained for an optimized silicon wafer.…
Production of silicon wafers comprises: (a) forming a silicon single crystal having an oxygen doping concentration of 4 x 10<17>/cm<3>, in which a molten material is solidified to a single crystal and cooling for 80 minutes at 850-1100 degrees C; (b) processing the…
A method is for the polishing of semiconductor wafers, which are mounted on a front side of a support plate and one side face of which is pressed anst a polishing plate, which is covered with a polishing cloth, with a specific polishing pressure and polished. A device is…
A process and device for polishing semiconductor wafers has at least one side of at least one semiconductor wafer pressed against a polishing plate, over which a polishing cloth is stretched. The semiconductor wafer and the polishing plate are moved relative to each other to…
Device for pulling a silicon single crystal 1 includes an element 5 which annularly surrounds the single crystal growing at a crystallization boundary; and the element has a face 6 directed at the single crystal. The element surrounds the single crystal substantially level with…
An apparatus and a method are provided for inspecting the edge micro-texture of a semiconductor wafer. The apparatus includes a diffuse hemisphere having at least one access port and has a normal axis, a laser target sphere mounted within the hemisphere, and a laser source…
A process for the double-side polishing of semiconductor wafers between two polishing plates which rotate in opposite directions and are covered with polishing cloth, so that at least 2 μm of semiconductor material is removed. The semiconductor wafers lay in plastic-lined…
PROBLEM TO BE SOLVED: To effectively avoid flaws to be linked to heating of a work. SOLUTION: A method for cutting off a work is provided wherein in a method for cutting off a rod-like or block-like work by using a saw, a temperature of the work is measured during cutting-off,…
A method to convert a reclaim wafer into a semiconductor wafer, suitable as starting material for semiconductor fabrication, with a front surface, a back surface and an edge. At least one of the two surfaces bearing foreign material which originates from at least one process for…
A process for producing semiconductor wafers by double-sided polishing between two rotating, upper and lower polishing plates, which are covered with polishing cloth, while an alkaline polishing abrasive with colloidal solid fractions is being supplied, the semiconductor wafers…
A carrier for a semiconductor wafer has at least three protrusions on whichhe edge of the semiconductor wafer is supported so that the semiconductor wafer is positioned essentially horizontal. The carrier does not make contact with the front side and the rear side of the…
A method and device for detecting an incorrect position of a semiconductor wafer during a high-temperature treatment of the semiconductor water in a quartz chamber which is heated by IR radiators, has the semiconductor wafer lying on a rotating support and being held at a…
Producing a semiconductor wafer comprises polishing the edges of the wafer with a cloth with the continuous introduction of an alkaline polishing agent; simultaneously polishing the front and rear sides of the wafer with continuous introduction of an alkaline polishing agent…
A semiconductor wafer has extremely low front face site front surface-referenced least squares ratio (SFQR) values varying insignificantly between the wafer edge and central regions. Semiconductor wafer has a front face with a maximum local planarity value (SFQRmax) of <=…
<P>PROBLEM TO BE SOLVED: To obtain a cost advantage as compared with a case using a carrier and method by known prior art, especially by reducing a scratching rate in a work in an initial stage of using the new carrier. <P>SOLUTION: A side surface 10 of another notch…