An Al 3 Ti film having a large amount of dissolved Si is deposited on a semiconductor substrate to form a laminate with an Al wiring film, and heat treatment is performed at a temperature of at least 400° C., to thereby absorb excessive Si into the Al 3 Ti film and to so prevent…
Assignee / Organization
Usami Tetsuo
1Total Forward Citations
1Indexed Patents
1Avg Citations / Patent
1Portfolio H-Index
Key Inventors: Arakawa Yoshikazu Usami Tetsuo