WO 2014/074622 A1#6443390 Most Cited · 15 citations1.2/yr · PR 2.17PendingWO · Application
Low density polyolefin resins ad films made therefrom

Disclosed herein are broad molecular weight distribution olefin polymers having densities in the 0.895 to 0.930 g/cm 3 range, and with improved impact and tear resistance. These polymers can have a ratio of Mw/Mn in the 8 to 35 range, a high load melt index in the 4 to 50 range,…

WO 2012/040144 A1#12800325 Most Cited · 8 citations0.6/yr · PR 2.33PendingWO · Application
Novel catalyst systems and polymer resins having improved barrier properties

A unimodal polymeric resin having a density of from about 0.946 g/ml to about 0.97 g/ml and a zero shear viscosity of from about 8 x 10 2 Pa-s to about 6 x 10 4 Pa-s. A method comprising (a) providing a catalyst system comprising a half-sandwich transition metal complex; (b)…

WO 2012/030779 A1#28328422 Most Cited · 3 citations0.2/yr · PR 1.55PendingWO · Application
Polymer resins having improved barrier properties and methods of making same

A polymeric resin having a lower molecular weight (LMW) component and a higher molecular weight (HMW) component and the resin having a density of from about 0.955 g/cc to about 0.967 g/cc, a melt index of from about 0.5 dg/min to about 4.0 dg/min, and a zero shear viscosity of…

WO 2010/080106 A1#45863085 Most Cited · 1 citations0.1/yr · PR 1.49PendingWO · Application
Process for producing broader molecular weight distribution polymers with a reverse comonomer distribution and low levels of long chain branches

The present invention provides a polymerization process which is conducted by contacting an olefin monomer and at least one olefin comonomer in the presence of hydrogen and a metallocene-based catalyst composition. Polymers produced from the polymerization process are also…

WO 2019/067270 A1#56398545 Most Cited · 1 citations0.1/yr · PR 0.80PendingWO · Application
Dual component lldpe copolymers with improved impact and tear resistance

Disclosed are ethylene polymer compositions containing a homogeneously-branched first ethylene polymer component and a homogeneously-branched second ethylene polymer component of higher density than the first ethylene polymer component. The ethylene polymer composition can be…

EP 3,692,082 A1#95910818 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Dual catalyst system for producing lldpe copolymers with improved processability

Disclosed herein are ethylene-based polymers generally characterized by a density from 0.89 to 0.93 g/cm3, a ratio of Mw/Mn from 3 to 6.5, a Mz from 200,000 to 650,000 g/mol, a CY-a parameter at 190°C from 0.2 to 0.4, and a reverse short chain branching distribution. The ATREF…

WO 2018/194881 A1#67271377 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Novel polyethylene compositions and methods of making and using same

A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590 °F to about 645 °F and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0…

WO 2019/070440 A1#132543117 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Dual catalyst system for producing lldpe copolymers with improved processability

Disclosed herein are ethylene-based polymers generally characterized by a density from 0.89 to 0.93 g/cm 3, a ratio of Mw/Mn from 3 to 6.5, a Mz from 200,000 to 650,000 g/mol, a CY-a parameter at 190°C from 0.2 to 0.4, and a reverse short chain branching distribution. The ATREF…