Provided is an epitaxial wafer manufacturing method wherein a carbon implanted layer is formed by implanting carbon ions, then, heat treatment is performed in an atmosphere containing ammonia or nitrogen by using a rapid heating/cooling (RTA) apparatus, and an epitaxial layer is…
Tobe Satoshi
Silicon epitaxial wafer (100) comprises silicon single-crystal substrate (1) produced by the CZ process and doped with boron so as to exhibit a resistivity of ≤ 0.018 Ω·cm and, superimposed thereon, silicon epitaxial layer (2). In the silicon single-crystal substrate (1) as a…
Provided is an insulating film forming method wherein an insulating film is formed by performing heat treatment to a silicon wafer in an atmosphere gas. In the method, oxygen diluted with nitrogen is used as the atmosphere gas. The heat treatment is performed to the silicon…
Provided are a thin film silicon wafer having high gettering capability, a manufacturing method therefor, a multi-layered silicon wafer formed by laminating the thin film silicon wafers, and a manufacturing method therefor. The thin film silicon wafer is manufactured by: forming…
A heat treatment method for suppressing slip dislocation even under the high-temperature heat treatment of a CZ silicon single crystal wafer with a diameter of mainly 300mm or more, and for sufficiently annihilating Grown in defects in a vicinity of the surface. An anneal wafer…
Silicon epitaxial wafer (100) comprising silicon single crystal substrate (1) produced by the CZ process and doped with boron so as to exhibit a resistivity of 0.009 to 0.012 Ω·cm and, provided thereon, silicon epitaxial layer (2). In the silicon single crystal substrate (1)…
A heat treating method capable of increasing a BMD density and expanding a DZ layer width, and a silicon wafer having a larger DZ layer width than ever before despite its high BMD density. A silicon wafer containing interstitial oxygen is heat-treated (RTA treated) by a quick…
An epitaxial wafer comprising a silicon epitaxial layer formed on the surface of a nitrogen-doped silicon single-crystal wafer, characterized in that the oxygen deposit density of a size having a gettering power in a bulk is at least 108 pieces/cm3. A production method for an…
A silicon single crystal substrate (1) is manufactured by CZ method and is doped with boron to have a resistivity of 0.02 Ω·cm or less. On the silicon single crystal substrate, a silicon epitaxial layer (2) is vapor-phase grown, and low-temperature heat treatment is performed in…
Disclosed is a method for forming an oxide film for a silicon wafer, wherein the surface roughness of the silicon wafer and/or the crystallinity of the surface part of the silicon wafer are measured in advancem, the silicon wafer oxidation conditions are adjusted based on the…