Patents
Assignee / Organization

Sumitomo Titanium Corp

947Total Forward Citations
134Indexed Patents
7Avg Citations / Patent
17Portfolio H-Index
JP 2003128492 A#1161468 Most Cited · 44 citations1.9/yr · PR 13.00ExpiredJP · Utility
Method for producing polycrystalline silicon for semiconductor
Inventors: Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2001-10-23

PROBLEM TO BE SOLVED: To solve problems of deformation of a shape including a horizontal cross section, development of a popcorn and fluctuation of an outer diameter, not by ventilation from the upper part of a furnace nor using a multiple nozzle as is in conventional…

JP 2002241120 A#1517674 Most Cited · 38 citations1.6/yr · PR 6.78ExpiredJP · Utility
Reaction furnace for manufacturing polycrystalline silicon, and method of manufacturing polycrystalline silicon
Inventors: Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2001-02-15

PROBLEM TO BE SOLVED: To prevent the deterioration of horizontal cross-sectional shape of a polycrystalline silicon rod manufactured by a siemens method, to prevent the occurrence of ruggedness on the surface of the polycrystalline rod and to enhance the availability of a…

JP 2004149351 A#1534323 Most Cited · 38 citations1.7/yr · PR 5.10ExpiredJP · Utility
Chlorosilane and method for purifying the same
Inventors: Okamoto NoboruAssignee: Sumitomo Titanium CorpFiled 2002-10-30

<P>PROBLEM TO BE SOLVED: To provide trichlorosilane that is capable of effecting the reduction of a concentration of carbon impurities to the conventional level or less at a relatively low cost, and to provide a method for purifying the same. <P>SOLUTION: A…

JP 2006016243 A#1505322 Most Cited · 38 citations1.9/yr · PR 9.26ExpiredJP · Utility
Method for manufacturing polycrystalline silicon and seed holding electrode
Inventors: Yamamoto KenjiAssignee: Sumitomo Titanium CorpFiled 2004-07-01

<P>PROBLEM TO BE SOLVED: To provide a method for manufacturing polycrystalline silicon, which contributes to the reduction of the electric power cost and realizes the improvement in the quality and yield because the polycrystalline silicon or a member used in a seed…

US 2005214533 A1#1923554 Most Cited · 33 citations1.6/yr · PR 6.17PendingUS · Application
Photocatalytic composite material and method for preparation thereof

A photocatalytic composite material having a high activity and good durability is produced by coating the surface of a substrate with a continuous film of titanium oxide by vapor deposition from titanium tetrachloride. In the case of a substrate which is a mass of inorganic…

JP 2004071456 A#2252050 Most Cited · 30 citations1.4/yr · PR 5.45ExpiredJP · Utility
Porous conductive plate

<P>PROBLEM TO BE SOLVED: To provide a porous conductive plate that is superior in forming performance as well as in contacting performance with a membrane electrode jointing body and has little danger of damaging the membrane electrode jointing body. <P>SOLUTION:…

JP 2005112662 A#2496190 Most Cited · 28 citations1.3/yr · PR 6.15ExpiredJP · Utility
Polycrystalline silicon rod and method of manufacturing the same
Inventors: Yamamoto Kenji, Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2003-10-07

<P>PROBLEM TO BE SOLVED: To provide a polycrystalline silicon rod exhibiting excellent crack resistance when receiving thermal stress. <P>SOLUTION: In the manufacture of the polycrystalline silicon rod by a Siemens method using a silicon core material and silanes as…

JP 2006089353 A#2496752 Most Cited · 28 citations1.4/yr · PR 6.11ExpiredJP · Utility
Polycrystalline silicon and its manufacturing method
Inventors: Yamawaki KenjiAssignee: Sumitomo Titanium CorpFiled 2004-09-27

<P>PROBLEM TO BE SOLVED: To provide a polycrystalline silicon capable of decreasing the contamination of a resin powder during transportation, and a method of manufacturing the polycrystalline silicon efficiently. <P>SOLUTION: This polycrystalline silicon has an…

JP 2004275999 A#2609521 Most Cited · 27 citations1.2/yr · PR 12.35ExpiredJP · Utility
Titanium oxide-based photocatalyst, manufacturing method therefor and its application

<P>PROBLEM TO BE SOLVED: To provide a photocatalyst which stably exhibits a high photocatalytic action under visible light irradiation and which is easily mass-produced. <P>SOLUTION: The metal halide-containing titanium oxide-based photocatalyst is obtained by…

JP 2003306789 A#3395887 Most Cited · 23 citations1.0/yr · PR 4.60ExpiredJP · Utility
Method and apparatus for manufacturing sponge titanium
Inventors: Uedahira Takashi, Nakamura YoshioAssignee: Sumitomo Titanium CorpFiled 2002-04-19

<P>PROBLEM TO BE SOLVED: To provide a method and an apparatus by which the concentration of molten salt incorporated in electrolytic magnesium which causes the diminishing of yield of sponge titanium is reduced in the manufacturing method of sponge titanium by the…

JP 2004068112 A#3440048 Most Cited · 23 citations1.1/yr · PR 3.74ExpiredJP · Utility
Electroconductive porous plate

<P>PROBLEM TO BE SOLVED: To provide an electroconductive porous plate which is easily manufactured and highly economic, shows an excellent moldability and surface smoothness and exerts no drastic change in properties in its thickness direction. <P>SOLUTION: The…

JP 2006001804 A#3390685 Most Cited · 23 citations1.1/yr · PR 4.73ExpiredJP · Utility
Method of manufacturing silicon chloride and method of manufacturing polycrystalline silicon using the same
Inventors: Matsunaga ShozoAssignee: Sumitomo Titanium CorpFiled 2004-06-18

<P>PROBLEM TO BE SOLVED: To provide a method of manufacturing silicon chlorides, in which metallic silicon, wherein the aluminum concentration is higher than that in the conventional metallic silicon, is used as a raw material, and to provide a method of manufacturing…

JP 2002210355 A#3601689 Most Cited · 22 citations0.9/yr · PR 5.11ExpiredJP · Utility
Rod dismounting apparatus
Inventors: Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2001-01-18

PROBLEM TO BE SOLVED: To provide a rod dismounting apparatus capable of carrying out a set of two silicon rods, which is standing close together in a massed state in a vapor growing furnace for preparing a polycrystal silicon rods for semiconductors, outside the furnace…

JP 2002293688 A#4135270 Most Cited · 20 citations0.8/yr · PR 4.69ExpiredJP · Utility
Method of detecting contamination during cleaning of polycrystalline silicon for semiconductor and method of cleaning the same as well as pure water cleaning equipment for the same
Inventors: Yamawaki KenjiAssignee: Sumitomo Titanium CorpFiled 2001-12-11

PROBLEM TO BE SOLVED: To provide an apparatus capable of surely detecting carbon-base inclusions of fine powder during cleaning or inspecting in production of polycrystalline silicon which is raw material for semiconductors, a method for detecting the same as well as pure water…

JP 2004349237 A#4063242 Most Cited · 20 citations0.9/yr · PR 14.13ExpiredJP · Utility
Cathode for lithium secondary battery, lithium secondary battery using cathode, deposition material used for cathode formation, and manufacturing method of cathode
Inventors: Natsume YoshitakeAssignee: Sumitomo Titanium CorpFiled 2003-08-19

<P>PROBLEM TO BE SOLVED: To greatly improve the low level of an initial efficiency as its shortcoming without impairing the large level of an initial charge capacity which is a characteristic of a lithium secondary battery using SiO as a negative electrode.…

JP 2002339006 A#4750343 Most Cited · 18 citations0.8/yr · PR 5.46ExpiredJP · Utility
Method for manufacturing titanium and titanium alloy powder
Inventors: Arimoto NobuhiroAssignee: Sumitomo Titanium CorpFiled 2001-05-15

PROBLEM TO BE SOLVED: To provide a method for manufacturing fine titanium powder and titanium-alloy powder of minimal contamination by a gas atomizing method. SOLUTION: In this method, the titanium powder and the titanium alloy powder can be manufactured by the gas atomizing…

JP 2003306321 A#4724065 Most Cited · 18 citations0.8/yr · PR 7.26ExpiredJP · Utility
Polycrystalline silicon and its manufacturing method
Inventors: Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2002-04-11

<P>PROBLEM TO BE SOLVED: To easily and economically manufacture a polycrystalline silicon which can prevent a processing crack in machining when used as a raw material for additional charge for manufacturing a silicon single crystal with CZ method (Czochralski method).…

JP 2004277223 A#4817020 Most Cited · 18 citations0.8/yr · PR 3.99ExpiredJP · Utility
High strength polycrystalline silicon and its manufacturing method
Inventors: Ochiai SanjiAssignee: Sumitomo Titanium CorpFiled 2003-03-17

<P>PROBLEM TO BE SOLVED: To provide a polycrystalline silicon rod having high strength and excellent cracking resistance. <P>SOLUTION: In the process of manufacturing a polycrystalline silicon rod from silanes as the source material by Siemens method, the surface…

US 7,297,271 B2#4993737 Most Cited · 18 citations0.9/yr · PR 2.56ActiveUS · Utility
Titanium powder sintered compact
Inventors: Onishi Takashi, Ogasawara Tadashi, Watanabe Munetoshi, Kato MasamichiAssignee: Sumitomo Titanium CorpFiled 2006-08-10 · Granted 2007-11-20

Provided are a porous sintered compact suitable for a filter, a power feeder in a polymer electrolyte membrane type water electrolyzer, a current collector in a solid polymer fuel cell and in addition a liquid dispersion plate, especially an ink dispersion plate for an ink jet…

JP 2006169012 A#5201201 Most Cited · 17 citations0.8/yr · PR 3.92ExpiredJP · Utility
Hexachlorodisilane and method of producing the same
Inventors: Okamoto NoboruAssignee: Sumitomo Titanium CorpFiled 2004-12-13

<P>PROBLEM TO BE SOLVED: To produce hexachlorodisilane (Si<SB>2</SB>Cl<SB>6</SB>) with which the yield in the production of silicon fluoride (Si<SB>2</SB>F<SB>6</SB>) is improved. <P>SOLUTION: Hexachlorodisilane…

US 7,014,722 B1#5380747 Most Cited · 17 citations0.8/yr · PR 2.65ExpiredUS · Utility
Titanium material superior in upset-forgeability and method of producing the same
Inventors: Arimoto Nobuhiro, Ogasawara Tadashi, Uemura Isao, Mitani Youji, Oonishi TakashiAssignee: Sumitomo Titanium CorpFiled 2000-08-10 · Granted 2006-03-21

In finifsh-cogging a high-purity titanium material into a cylindrical form as the final shape, if cylindrical cogging is performed in all stages of warm forging or if cylindrical cogging is performed in the initial stage of the warm forging, there is no need of peripherally…

WO 2006/011290 A1#5136617 Most Cited · 17 citations0.8/yr · PR 5.15PendingWO · Application
SiO POWDER FOR SECONDARY BATTERY AND PROCESS FOR PRODUCING THE SAME

An SiO powder for secondary battery that is used as a negative electrode material of lithium secondary battery and characterized in that the concentration of contained hydrogen is ≥ 80 ppm. The powder would enable striking enhancement of discharge capacity and rate of cycle…

JP 2003095635 A#5646895 Most Cited · 16 citations0.7/yr · PR 3.70ExpiredJP · Utility
Manufacturing device for polycrystalline silicon
Inventors: Matsunaga ShozoAssignee: Sumitomo Titanium CorpFiled 2001-09-27

PROBLEM TO BE SOLVED: To recover hydrogen gas from exhaust gas generated in a reaction furnace where polycrystalline silicon is manufactured from mixed gas of a chlorosilane and hydrogen with a vapor phase reducing method and to prevent pipe-clogging, machine damage, etc., due…

JP 2007044763 A#5628456 Most Cited · 16 citations0.8/yr · PR 3.89ActiveJP · Utility
Method for producing titanium material for sputtering
Inventors: Yoshino Masaki, Yoshikawa ShogoAssignee: Sumitomo Titanium CorpFiled 2006-01-13

<P>PROBLEM TO BE SOLVED: To provide a titanium material for sputtering in which a cast ingot is used as a starting raw material, and this titanium material has clean macro-structure and fine micro-structure and the defect on a surface layer is little and good upsetting…