An illumination system for a micro-lithographic contact and proximity exposure apparatus comprising a light source (1), a collector (2), two optical integrators (3,6), two Fourier lenses (4,7), at least one angle defining element (5); and at least one field lens (8). The first…
Suess Microtec Lithography
The invention relates to a method for aligning two flat substrates with one another, wherein each substrate has at least one aligning mark for mutual alignment, particularly for aligning a mask with a wafer before exposure. After aligning the two substrates in a first aligning…
The present application describes a method and a device for keeping the mask dimensions of a mask ( 6 ) constant in the mask plane in lithography. The mask ( 6 ) is heated due to the exposure during lithography. By means of thermal and/or mechanical methods, the dimensions of…
The bonding method has 2 wafers (1,2) aligned with one another to form a stack and held in a first clamping device (11), with a spacer (12) positioned adjacent the latter before alignment of the third wafer (3) relative to the stacked wafers, with an opening (4) in the third…
Durch die Erfindung wird ein Verfahren zum Belacken von Substraten, insbesondere von Halbleitersubstraten, deren Oberfläche eine drei-dimensionale Topographie aufweisen, vorgeschlagen. Hierzu wird das Substrat mit einem mit einem Lösungsmittel modifizierten besprüht und…
Verfahren zur selektiven Plasmabehandlung mittels Barrierenentladung eines im Wesentlichen flächigen Substrats (1), insbesondere eines Halbleitersubstrats, zur Vorbehandlung vor einem Beschichtungs- oder Bondprozess mit den Schritten: (a) Anordnen einer dielektrischen Maske (2)…
The invention provides a method of lacquering substrates, in particular semiconductor substrates, whose surfaces have three-dimensional topographies. For this purpose, the substrate is sprayed with a lacquer that is modified with a solvent, and subsequently the applied lacquer…
A method of determining the bond strength between two bonded substrates comprises placing a knife (3) at the circumference of the substrates at the bonding surface (12), pushing the knife between the substrates, determining the path and force during penetration between the…
The invention provides a method for determining the center of a rotationally symmetrical alignment mark thereby using an image recognition software. The alignment mark is recognized by the image recognition software in different orientations by rotating the alignment mark around…
A rotationally symmetric alignment mark (J) centre (M) determination procedure uses image recognition software to fix the positions of a reference point (R1, R2) in images rotated (JO) through its angle of symmetry one or more times.
Process for pre-treating surfaces or bonding surfaces of substrates (1, 1') to be joined comprises applying an atmospheric plasma before the bonding process is carried out. An Independent claim is also included for a device for pre-treating the surfaces or bonding surfaces…
Durch die vorliegende Erfindung wird eine Vorrichtung bzw. ein Chuck zum Fixieren von dünnen und/oder flexiblen Substraten bereitgestellt, der ein gleichmäßiges und vollflächiges Ansaugen der Substrate ohne nachteiliges Verziehen oder Verbiegen ermöglicht. Der Chuck weist Nuten…
PROBLEM TO BE SOLVED: To provide an improved device for temporary wafer bonding.SOLUTION: An improved device for temporary wafer bonding includes a temporary bonder cluster and debonder cluster. The temporary bonder cluster includes a temporary bonder module performing…
Process for joining at least two semiconductor substrates (1) comprises moving a radiation source (3) relative to a bonding surface (1a) during pretreatment. An independent claim is also included for a device for pretreating bonding surfaces before bonding.
Selective plasma treatment of a flat substrate (1), especially a semiconductor substrate, as a pre-treatment prior to application of a coating or prior to a bonding process involving:(a) arrangement of a dielectric mask (2), i.e. a glass layer less than 5 mm thick, at a distance…
Verfahren zum Belacken eines Substrats mit den Schritten: (a) Modifizieren des aufzubringenden Lacks mit einem Lösungsmittel; (b) Versprühen des modifizierten Lacks auf das Substrat; und (c) Homogenisieren der aufgesprühten Lackschicht in einer Lösungsmittelatmosphäre, wobei die…
The device has a field lens and a set of solid state device ultra violet light sources (15) that emit light with wavelength that ranges between 250 nanometers and 450 nanometers. The solid state ultra violet light sources are individually controllable and are arranged on a…
An apparatus for removing an adhesive layer from a wafer surface includes a chuck, a contact roller, a pick-up roller and a detaping tape. The chuck is configured to support and hold a wafer that comprises an adhesive layer on its top surface. The contact roller comprises an…
The invention relates to a method for non-drip dispensing of a liquid by means of a nozzle (1) onto a substrate (4), wherein said method comprises the following steps: dispensing the liquid from a first channel (2) of the nozzle onto the substrate, stopping dispensing the liquid…
The invention relates to an illumination unit (1) for a mask aligner. The illumination unit (1) comprises a light source (2), which may sequentially generate reasonable light distribution in the illumination plane (13) for nearly any mask aligner by means of a multi-axial…
The invention relates to a method and a device for keeping the dimensions of a mask (6) in the mask plane constant during lithography. The mask (6) is heated by exposure during lithography. The dimensions of the mask (6) are kept constant using thermal and/or mechanical methods.…