US 2006093809 A1#1455273 Most Cited · 39 citations1.9/yr · PR 6.34PendingUS · Application
Optical bodies and methods for making optical bodies

Optical bodies are disclosed that include an optical film and at least one rough strippable skin layer operatively connected to a surface of the optical film. The at least one rough strippable skin layer can include a continuous phase and a disperse phase. Alternatively, the at…

US 2004219338 A1#2272619 Most Cited · 30 citations1.4/yr · PR 4.52PendingUS · Application
Materials, configurations, and methods for reducing warpage in optical films

A multilayer optical body having improved dimensional stability is disclosed. The optical body includes an optical film, such as an oriented multilayer optical film, and a dimensionally stable (warp-resistant) layer that includes a combination of i) polystyrene or a first…

US 2006093846 A1#2303837 Most Cited · 30 citations1.5/yr · PR 3.38PendingUS · Application
Optical films incorporating cyclic olefin copolymers

A norbornene-based cyclic olefin layer with a curable layer disposed thereon is described. The curable layer may additionally be imparted with a texture. The norbornene-based cyclic olefin films with curable layers can be incorporated into optical bodies which include an optical…

US 2003105176 A1#2382178 Most Cited · 29 citations1.3/yr · PR 5.12PendingUS · Application
Foam and method of making

The present invention is directed to a process for producing a polypropylene foam by mixing a high melt strength polypropylene and a blowing agent to form a melt mixture, reducing the temperature of the melt mixture at the exit of the apparatus to an exit temperature that is no…

US 2006093845 A1#4923261 Most Cited · 18 citations0.9/yr · PR 3.05PendingUS · Application
Optical films incorporating cyclic olefin copolymers

A norbomene-based cyclic olefin layer with a curable layer disposed thereon is described. The curable layer may additionally be imparted with a texture. The norbomene-based cyclic olefin films with curable layers can be incorporated into optical bodies which include an optical…

US 2004155372 A1#5405928 Most Cited · 17 citations0.8/yr · PR 2.50PendingUS · Application
Process for manufacturing polymeric optical film

A process for making an optical film includes stretching a polyolefin film in a first direction and stretching the polyolefin film in a second direction different than the first direction forming a biaxially stretched polyolefin film. At least a portion of the stretching of the…

US 2006159888 A1#5908774 Most Cited · 16 citations0.8/yr · PR 2.22PendingUS · Application
Optical films incorporating cyclic olefin copolymers

The present disclosure relates to optical bodies including one or more norbornene-based cyclic olefin film layers and one or more rough strippable skin layers operatively connected to a surface of the norbornene-based cyclic olefin film layer. The rough strippable skin layer…

WO 0,200,412 A2#6843032 Most Cited · 14 citations0.6/yr · PR 2.80PendingWO · Application
Foam and method of making

The present invention is directed to a process for producing a polypropylene foam by mixing a high melt strength polypropylene and a blowing agent to form a melt mixture, reducing the temperature of the melt mixture at the exit of the apparatus to an exit temperature that is no…

US 2004156106 A1#7538530 Most Cited · 13 citations0.6/yr · PR 2.62PendingUS · Application
Polymeric optical film

An optical film includes a layer of simultaneous biaxially stretched polyolefin film that is substantially non-absorbing and non-scattering for at least one polarization state of visible light. The layer has x, y, and z orthogonal indices of refraction where at least two of the…

US 2004156000 A1#8569331 Most Cited · 12 citations0.6/yr · PR 2.01PendingUS · Application
Compensators for liquid crystal displays

An optical stack includes a first liquid crystal layer and a j-retarder disposed on the liquid crystal layer. The j-retarder includes a simultaneous biaxally stretched polymeric film being substantially non-absorbing and non-scattering for at least one polarization state of…

US 2003211310 A1#10537625 Most Cited · 10 citations0.4/yr · PR 1.99PendingUS · Application
Foam and method of making

The present invention is directed to a process for producing a polypropylene foam by mixing a high melt strength polypropylene and a blowing agent to form a melt mixture, reducing the temperature of the melt mixture at the exit of the apparatus to an exit temperature that is no…

US 2006228592 A1#9999274 Most Cited · 10 citations0.5/yr · PR 2.86PendingUS · Application
Optical bodies including rough strippable boundary layers

Optical bodies are disclosed that include a first optical film, a second optical film and at least one rough strippable boundary layer disposed between the first and second optical films. Also disclosed are optical bodies including a strippable boundary layer disposed between…

WO 0,031,202 A1#53357398 Most Cited · 1 citations0.0/yr · PR 0.82PendingWO · Application
Backing for adhesive tape and such tape

Films useful as tape backings, and more particularly biaxially oriented polypropylene film backings and tapes including such backings. A brittle, biaxially oriented polypropylene film is provided by minimizing the nucleation density in the extruded and quenched polypropylene…

WO 2004/072712 A2#54944644 Most Cited · 1 citations0.1/yr · PR 0.81PendingWO · Application
Process for manufacturing polymeric optical film

A process for making an optical film includes stretching a polyolefin film in a first direction and stretching the polyolefin film in a second direction different than the first direction forming a biaxially stretched polyolefin film. At least a portion of the stretching of the…

US 8,568,869 B2#72339782 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Optical bodies including rough strippable boundary layers and asymmetric surface structures

Optical bodies are disclosed that include an optical film and at least one rough strippable skin layer. The at least one rough strippable skin layer can include a continuous phase and a disperse phase. In some embodiments, the at least one rough strippable skin layer can include…

US 9,709,700 B2#115162008 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredUS · Utility
Optical bodies including rough strippable boundary layers

Optical bodies are disclosed that include a first optical film, a second optical film and at least one rough strippable boundary layer disposed between the first and second optical films. Also disclosed are optical bodies including a strippable boundary layer disposed between…

WO 0,200,412 A3#114962159 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Foam and method of making

The present invention is directed to a process for producing a polypropylene foam by mixing a high melt strength polypropylene and a blowing agent to form a melt mixture, reducing the temperature of the melt mixture at the exit of the apparatus to an exit temperature that is no…

WO 2004/072701 A1#75602158 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Polymeric optical film

An optical film includes a layer of simultaneous biaxially stretched polyolefin film that is substantially non-absorbing and non-scattering for at least one polarization state of visible light. The layer has x, y, and z orthogonal indices of refraction where at least two of the…

WO 2004/072712 A3#71105710 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Process for manufacturing polymeric optical film

A process for making an optical film includes stretching a polyolefin film in a first direction and stretching the polyolefin film in a second direction different than the first direction forming a biaxially stretched polyolefin film. At least a portion of the stretching of the…

WO 2004/072718 A1#64507315 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Compensators for liquid crystal displays

An optical stack (300) includes a first liquid crystal layer (320) and a retarder (310) disposed on the liquid crystal layer. The retarder includes a simultaneous biaxially stretched polymeric film being substantially non-absorbing and non-scattering for at least one…