A dispersion optimized fiber comprising a centre core, two side cores, a cladding and a outer glass, wherein first side core is provided onto outer periphery of center core, second side core is provided onto outer periphery of first side core and cladding region is provided onto…
Sterlite Optical Technologies
Dispersion shifted fiber having low dispersion slope comprising a center core, two claddings, a ring core and the outer glass region, wherein the first cladding is provided onto the outer periphery of the center core, the second cladding is provided onto outer periphery of the…
A dispersion optimized optical fiber for wideband optical transmission is disclosed. The fiber comprises centre core, inner cladding, ring core, outer cladding and outer glass region, characterized by inner cladding provided onto outer periphery of the centre core, ring core…
A method for manufacturing an optical fiber having uniform refractive index profile, and substantially reduced macrobending loss and attenuation loss is provided comprising controlling one or more of parameters including concentration of dopant in outer region and inner region…
A method for manufacturing a multimode optical fiber having higher bandwidth comprising applying correction factor to obtain desired layerwise alpha refractive index profile thereby resulting in formation of the preform to form an optical fiber having higher bandwidth. The…
The present invention relates to a method of preparing low attenuation single mode fiber and particularly to the preparation of optical fiber preform from which single mode optical fiber is drawn shows low transmission loss in the 1360 to 1460 nm (E-band) wavelength region.
A method for producing optical fiber having reduced hydrogen induced loss is provided wherein the optical fiber is treated with deuterium gas for a predetermined duration. The predetermined duration of deuterium treatment is determined based on three factors, that is, a) the…
A dispersion optimized fiber having higher spot area comprising a center core region, a cladding region, a ring core region and an outer glass region is provided, wherein the cladding is provided onto the outer periphery of the center core, and the ring core is provided onto the…
The invention provides a method for producing optical fiber having reduced hydrogen induced loss wherein the optical fiber is treated with deuterium gas for a predetermined duration. The predeterminedduration of deuterium treatment is determined based on three factors, that is,…
A method for producing an optical fiber preform having a large size soot porous body is provided wherein opposite ends of the rod are heated by heating means to achieve a predetermined temperature which is increased in a controlled manner in a stepwise mode or a gradual mode or…
A method for drawing an optical fiber having reduced polarization mode dispersion (PMD) draws an optical fiber from an optical fiber preform whose core ovality is at max about 3%, coats the optical fiber with acrylic polymer and twists the coated optical fiber with a pair of…
A rotary seal capable of joining a stationary member with a rotating member is provided, wherein the rotary seal comprises a body having a central hole therethrough, wherein said central hole has stepwise reducing diameter so as to form two part central hole, wherein front part…
Dispersion shifted fiber having low dispersion slope comprising a centre core, two claddings, a ring core and the outer glass region, wherein the first cladding is provided onto the outer periphery of the centre core, the second cladding is provided onto outer periphery of the…
The present invention relates to a method of manufacturing a solid glass preform (103) from which single mode optical fiber is drawn showing low transmission loss in the 1360 to 1460 nm (E-band) wavelength region. The method comprises the steps of depositing porous silica based…
A method for producing optical fiber having reduced hydrogen induced loss is provided wherein the optical fiber is treated with deuterium gas for a predetermined duration. The predetermined duration of deuterium treatment is determined based on three factors, that is, a) the…
A rotary seal capable of joining a stationary member with a rotating member is provided, wherein the rotary seal comprises a body having a central hole therethrough, wherein said central hole has stepwise reducing diameter so as to form two part central hole, wherein front part…
A method for producing an optical fiber having desired cutoff wavelength, mode field diameter [MFD] and zero dispersion wavelength [ZDW] waveguide parameters even when actual refractive index [RI] profile has various configurations is provided. The method comprises…
An apparatus and method for drawing a fiber having desired waveguide parameters, particularly cut-off wavelength is provided. The apparatus is characterized by a temperature measurement means (113) provided near surface (A) of the preform (105), being capable of directly…
An apparatus and method for drawing an optical fiber is provided. Apparatus comprises a furnace comprising a furnace chamber with heating elements, a preform is suspended in core tube of the furnace for heating its tip, diffuser having an orifice at the top face of furnace…
A process for producing optical fiber preform having symmetrically and completely collapsed capillary which is suitable for producing optical fiber having reduced PMD is provided, wherein collapsing of the capillary in the hollow soot porous body or sintered glass body is…
A method for producing an optical fiber preform having a large size soot porous body is provided wherein opposite ends of the rod are heated by heating means to achieve a predetermined temperature which is increased in a controlled manner in a stepwise mode or a gradual mode or…
A rotary seal (20) capable of joining a stationary member (21) with a rotating member (22) is provided, wherein the rotary seal comprises a body (23) having a central hole (24) therethrough, wherein said central hole (24) has stepwise reducing diameter so as to form two part (25…
A process for preparing the mandrel suitable for producing flawless optical fiber preform, wherein the mandrel can be easily removed from the soot porous body without causing any defects, such as voids, bubbles, impurities, uncollapsed portion in the centerline region of the…
Dispersion shifted fiber having low dispersion slope comprising a centre core, two claddings, a ring core and the outer glass region, wherein the first cladding is provided onto the outer periphery of the centre core, the second cladding is provided onto outer periphery of the…
A method for manufacturing an optical fiber having uniform refractive index profile, and substantially reduced macrobending loss and attenuation loss is provided comprising controlling one or more of parameters including concentration of dopant in outer region and inner region…