In a method for casting a piston for an internal combustion engine, after solidification of the surface layer in the region of the piston-pin bores ( 12 ), at least one mandrel provided there is withdrawn and the region of at least one piston-pin bore ( 12 ) is cooled by coolant…
Assignee / Organization
Stephan Silvio
7Total Forward Citations
3Indexed Patents
2Avg Citations / Patent
2Portfolio H-Index
In a method for casting a piston for an internal combustion engine, after solidification of the surface layer in the region of the piston-pin bores ( 12 ), at least one mandrel provided there is withdrawn and the region of at least one piston-pin bore ( 12 ) is cooled by coolant…
In a method for casting a piston for an internal combustion engine, after solidification of the surface layer in the region of the piston-pin bores (12), at least one mandrel provided there is withdrawn and the region of at least one piston-pin bore (12) is cooled by coolant…