A method of making an investment shell mold in such a way that the shell is protected from cracking on simultaneous firing and removal of the pattern. The method includes application of conventional molding materials in the first slurry and stucco coats. By conventional molding…
Assignee / Organization
Stainless Foundry & Engineerin
69Total Forward Citations
9Indexed Patents
8Avg Citations / Patent
4Portfolio H-Index
False teeth, esp. arches and crowns, are cast from an alloy contg. 0.01-0.08% C, 26-28% Cr, 4-6.5% Ni, 5-8% Co, 1.8-3.8% Mo, 0.5-0.8% Si, 0.5-1.0% Mn, and the bal. Fe and melting impurities. Pref. compsn. is 0.04% C, 27.5% Cr, 5-2.% Ni, 6.5% Co, 2.3% Mo, 0.6% Si, 0.75% Mn, bal.…
A corrosion resistant alloy steel has the following percentage composition: .C.0.03-0.12 .Cr.24-28 .Ni.4-6.5 .Co.0.95-12 .Mo.1.75-3 .Si.0-1 .Mn.0-1.5 .Cu.0-0.5 .Fe the balance. The alloy may be silution treated at 1900-2050 DEG F. and aged at 850 DEG F.