The optical elements for ultraviolet radiation, especially for microlithography, are made from cubic granatite, cubic spinel, cubic perovskite and/or cubic M(II)- as well as M(IV)-oxides. The optical elements are made from suitable crystals of Y 3 Al 5 O 12 , Lu 3 Al 5 O 12 , Ca…
Staeblein Joerg
A method is described for making an especially not-(111)-oriented low-stress large-volume crystal having a glide plane with reduced stress birefringence and more uniform refractive index. The method includes growing and tempering the crystal while heating and/or cooling to form…
The method produces low-stress, large-volume crystals with low birefringence and uniform index of refraction. The method includes growing the crystal with larger than desired dimensions including diameter and height from a melt; cooling and tempering the crystal with the larger…
A method is described for making an especially not-(111)-oriented low-stress large-volume crystal having a glide plane with reduced stress birefringence and more uniform refractive index. The method includes growing and tempering the crystal while heating and/or cooling to form…
The method of making a single crystal, especially a CaF 2 single crystal, includes tempering, in which the crystal is heated at <18 K/h to a temperature of 1000° C. to 1350° C. and held at this temperature for at least 65 hours with maximum temperature differences within the…
The method produces highly uniform, low-stress single crystals, especially of calcium fluoride. A single crystal drawn from a melt apparatus with a suitable process is cooled and subsequently subjected to a tempering step. The method is characterized by rapid cooling in a…