A Sn—Ag—Cu based lead-free solder ball which does not undergo yellowing of its surface when formed into a solder bump on an electrode of an electronic part such as a BGA package. The solder ball has excellent wettability and does not form voids at the time of soldering, even…
Souma Daisuke
This invention provides a method for soldering an electroless Ni plating part that can overcome a disadvantage that, when an electrolessly Ni plated BGA electrode is soldered with solder balls of lead-free solder, the soldered part is disadvantageously easily separated upon…
An object of the present invention is to prevent “deteriorations,” such as oxidization and deformation of micro solder spheres during storage. The micro solder spheres are packed in a container 2 comprising an air permeable material. A deoxidizing and drying agent 3 to be…
A Sn-Ag-Cu based lead-free solder ball having a chemical composition, in mass %, that Ag: 1.0 to 4.0 %, Cu: 0.05 to 2.0 %, P: 0.0005 to 0.005 % and the balance: Sn. When used for forming a solder bump on the electrode of BGA or CSP, the above lead-free solder ball is free from…
[PROBLEMS] When Sn-Ag type, Sn-Cu type, Sn-Ag-Cu type and Sn-Sb type lead-free solder balls having a Sn content of 80 mass % or more were used for forming bumps on electrodes of BGA, the yellowing of the surface and/or the corrosion of the soldered portion in the case of…
An object of the present invention is to prevent “deteriorations,” such as oxidization and deformation of micro solder spheres during storage. The micro solder spheres are packed in a container 2 comprising an air permeable material. A deoxidizing and drying agent 3 to be…
Degradation of a minute solder ball during storage, such as oxidation or deformation, is prevented. Containers (2) formed from a breathable material are filled with minute solder balls. A deoxidizing desiccating agent (3) is prepared for application outside the containers (2).…