A copper alloy having an improved combination of yield strength and electrical conductivity consists essentially of, by weight, from 1% to 2.5% of nickel, from 0.5% to 2.0% of cobalt, with a total nickel plus cobalt content of from 1.7% to 4.3%, from 0.5% to 1.5% of silicon with…
Assignee / Organization
Seeger Joerg
1Total Forward Citations
3Indexed Patents
0Avg Citations / Patent
1Portfolio H-Index
A copper alloy having an improved combination of yield strength and electrical conductivity contains, by weight, from 1% to 2.5% of nickel, from 0.5% to 2.0% of cobalt, with a total nickel plus cobalt content of from 1.7% to 4.3%, from 0.5% to 1.5% of silicon with a ratio of…
The invention pertains to a process for producing a body consisting of an Al2O3/Al composite material and a body made by the process in question. First, a moulding is made from a mixture of an alkoxide solution, SiO2 powder and water. The moulding thus produced is then submerged…