A method for carburizing workpieces made of steel, particularly workpieces having outer and inner surfaces, the workpiece being held at a temperature in the range of 850 to 1050° C. in an atmosphere containing a gaseous hydrocarbon. At least two different gaseous hydrocarbons…
Schwarzer Jochen
The invention relates to a method for carbonitriding at least one component ( 12 ) in a treatment chamber ( 16 ), in which at least one process gas ( 28; 30 ) is introduced into the treatment chamber ( 16 ), wherein a hydrogen content ( 44 ) is detected in an atmosphere…
The invention relates to a method for carbonitriding at least one component (12) in a treatment chamber (16), in which at least one process gas (28; 30) is introduced into the treatment chamber (16), wherein a hydrogen content (44) is detected in an atmosphere developing in the…
In a method for carbonitriding at least one metal part, the metal part is heated in a heating phase to a treatment temperature, is nitrided in at least one nitriding phase using a nitrogen donor gas, and is carburized in at least one carburizing phase using a carbon donor gas.…
In a process for carbonitriding metallic components ( 1 ), provision is made of at least one carburization phase (C 1, C 2 ), in which the metallic component ( 1 ) is carburized with a carbon-donating gas. In addition, provision is made of a nitriding phase (C 1, C 2, C 3 ),…
The invention relates to a method for carbonitriding at least one metal part in which the metal part is heated to a treatment temperature in a heating phase (1), is nitrided with a nitrogen donor gas in at least one nitriding phase (2a-2d) and is carburized with a carbon donor…
In a process for carbonitriding metallic components (1), provision is made of at least one carburization phase (C1, C2), in which the metallic component (1) is carburized with a carbon-donating gas. In addition, provision is made of a nitriding phase (C1, C2, C3), which is…
A method for carburizing workpieces made of steel, particularly workpieces having outer and inner surfaces, the workpiece being held at a temperature in the range of 850 to 1050° C. in an atmosphere containing a gaseous hydrocarbon. At least two different gaseous hydrocarbons…
The invention relates to a method for carbonitriding at least one component ( 12 ) in a treatment chamber ( 16 ), in which at least one process gas ( 28; 30 ) is introduced into the treatment chamber ( 16 ), wherein a hydrogen content ( 44 ) is detected in an atmosphere…
The invention relates to a method for carburising steel workpieces, especially workpieces having outer and inner surfaces, whereby said workpiece is maintained at a temperature of between 850 and 1050°C in an atmosphere containing gaseous hydrocarbon. At least two different…
In a process for carbonitriding metallic components (1), provision is made of at least one carburization phase (C1, C2), in which the metallic component (1) is carburized with a carbon-donating gas. In addition, provision is made of a nitriding phase (C1, C2, C3), which is…
An installation for the dry transformation of a material microstructure of semi-finished products, especially for dry bainitization, includes a quenching chamber and a microstructure transformation chamber situated downstream from it in the processing flow, in each case the…
The present invention relates to an installation for the dry transformation of a material microstructure of semi-finished products, in particular for dry austempering, having a quenching chamber and a microstructure transformation chamber arranged at a later stage in the process…
The invention relates to a method for carburising steel workpieces, especially workpieces having outer and inner surfaces, whereby said workpiece is maintained at a temperature of between 850 and 1050°C in an atmosphere containing gaseous hydrocarbon. At least two different…
The invention relates to a method for carbonitriding at least one metal part in which the metal part is heated to a treatment temperature in a heating phase (1), is nitrided with a nitrogen donor gas in at least one nitriding phase (2a-2d) and is carburized with a carbon donor…