The present invention discloses an aluminosilicate glass and a glass ceramics for chemical tempering, specifically a novel aluminosilicate glass comprising Li 2 O and P 2 O 5 for chemical tempering. The glass of the present invention can have a high ion exchange rate by adding…
Schott Glass
The invention discloses aluminosilicate glass for chemical tempering and glass ceramics, and particularly discloses aluminosilicate glass which contains Li2O and P2O5 and can be chemically tempered. The glass of the invention can realize high ion exchange speed by the addition…
A strengthened high lanthanide-containing glass has the composition of, in mole percent ______________________________________ SiO 2 54-75 B 2 O 3 5-17 Li 2 O 0-4 Na 2 O 3-18 K 2 O 0-4 Al 2 O 3 0-7 PbO 0-4 MgO 0-3 CaO 0-3 SrO 0-3 BaO 0-3 ZnO 0.1-10 TiO 2 0-5 Ln 2 O 3 3-7 V 2 O 5…
A chemically toughened ultrathin glass is provided. The glass has a thickness less than 500 μm and a surface compressive layer having a depth of at most 30 μm. The toughened ultrathin glass sheet is more flexible and has extraordinary thermal shock resistance with the glass…
The invention discloses a method for producing tempered glass with a plurality of surface stress layers and a tempered glass product and particularly relates to a method for producing tempered lithium glass with a plurality of surface stress layers. The method comprises that a…
The invention relates to an aluminum silicate glass for a touch screen. The glass contains the following components in percentage by weight: 55-65 percent of SiO2, 12-17 percent of Na2O, 15-20 percent of Al2O3, 2-6 percent of K2O, 3.9-10 percent of MgO, 0-5 percent of ZrO2, 0-4…
A colored, chemstrengthenable contrast enhancement, UV attenuated glass (e.g., for sunglasses) comprises, in weight percent, ______________________________________ Oxide Wt. % ______________________________________ SiO 2 40-72 B 2 O 3 0-13 Al 2 O 3 0.5-3 Li 2 O 0-3 Na 2 O 8-13 K…
A strengthened high NdO 3 -containing glass has the composition of, in weight percent ______________________________________ SiO 2 40-60 Nd 2 O 3 10-30 As 2 O 3 /Sb 2 O 3 0-1 B 2 O 3 5.15 Na 2 O 3-18 ZnO 0.1-10 Li 2 O 0-3 K 2 O 0-3 Al 2 O 3 0-7 PbO 0-15 MgO 0-3 CaO 0-3 BaO 0-3…
A colored glass suitable for enhancing contrast of color CRT displays consists essentially of, in weight %: ______________________________________ SiO 2 40-60% B 2 O 3 0-6% Al 2 O 3 0-2% Sum Li 2 O + Na 2 O + K 2 O 24-30% Sum MgO + CaO + SrO + BaO + ZnO 0-10% TiO 2 1-3% CeO 2…
A low- or no-silica phosphate glass useful as a high average power laser medium and having a high thermal conductivity, K 90 ° C. >0.8 W/mK, and a low coefficient of thermal expansion, α 20 °-300° C. <90×10 -7 /°C., consisting essentially of (on a batch composition basis):…
In a high energy laser system utilizing phosphate laser glass components to amplify the laser beam, the laser system requires a generated laser beam having an emission bandwidth of less than 26 nm and the laser glass components consist essentially of (on an oxide composition…
A colored contrast enhancement glass comprises, in wt. %: ______________________________________ SiO 2 40-60 B 2 O 3 0-6 Al 2 O 3 0-2 ΣLi 2 O, Na 2 O, K 2 O = R 2 O 24-30 ΣMgO, CaO, SrO, ZnO, BaO = RO 0-10 TiO 2 1-3.5 CeO 2 1-3.5 Nd 2 O 3 4-12 La 2 O 3 1-11 MnO 2 0.1-1.0 Er 2 O…
A thin lithium-aluminosilicate glass is provided. The glass is suitable for three dimensional precision molding and suitable for toughening, wherein after toughening, the glass has a center tension smaller than 50 Mpa, a surface compressive stress of 600-1200 Mpa, and a bending…
Alkali-free borosilicate glass have been developed having coefficients of thermal expansion (+20° C. to +200° C.) below 40.5×10 -7 , densities less than 3.0 g/cm 3 and good visible and UV transmission, and can be produced by conventional continuous melting techniques. These…
A brown chemstrengthenable contrast enhancement, UV attenuated glass (e.g., for sunglasses) comprises, in weight percent, ______________________________________ Oxide Wt. % ______________________________________ SiO 2 40-72 B 2 O 3 0-13 Al 2 O 3 0.5-3 Li 2 O 0-3 Na 2 O 8-15 K 2…
The invention provides chemically tempered ultrathin glass, which is less than 500 microns in thickness and 30 microns at most in depth of a surface compression layer. The tempered ultra-thin glass sheet is more flexible and surprisingly resistant to thermal shock in the case of…
A low-or no-silica, low- or no-alkali phosphate glass useful as a laser amplifier in a multiple pass, high energy laser system having a high thermal conductivity, K 90 ° C. >0.85 W/mK, a low coefficient of thermal expansion, α 20 °-300° C. <80×10 -7 /°C., low emission…
A glass consisting essentially of (on an oxide composition basis): ______________________________________ Mole % ______________________________________ P 2 O 5 50-70 Al 2 O 3 4-13 Na 2 O 10-35 La 2 O 3 0-6 Ln 2 O 3 >0-6 Sum R'O 0-20 (R' = Mg, Ca, Sr, Ba, Zn and Pb)…
A low- or no-silica phosphate glass useful as a laser medium and having a high thermal conductivity, K 90 ° C. >0.8 W/mK, and a low coefficient of thermal expansion, α 20 °-40° C. <80×10 -7 /°C., consists essentially of (on a batch composition basis):…
The present invention provides a chemically toughened ultrathin glass, said glass has a thickness less than 500 μm, a surface compressive layer having a depth of at most 30 μm. Said toughened ultrathin glass sheet is more flexible and has extraordinary thermal shock resistance…
The invention relates to chemically tempered antimicrobial boroaluminosilicate glass free of color change. The boroaluminosilicate glass is characterized in that the content of B2O3 can meet the following relational expression as shown in the specification, wherein M2O is the…
An aluminosilicate glass for touch screens is provided. The glass includes, calculated based on weight percentage: SiO 2 , 55 to 65%; Na 2 O, 12 to 17%; Al 2 O 3 , 15 to 20%; K 2 O, 2 to 6%; MgO, 3.9 to 10%; ZrO 2 , 0 to 5%; ZnO, 0 to 4%; CaO, 0 to 4%; Na 2 O+K 2 O+MgO+ZnO+CaO,…
A Cu-doped/Fe-doped low expansion glass ceramic composition comprising: ______________________________________ Wt. % ______________________________________ SiO 2 50-65 Al 2 O 3 18-27 P 2 O 5 0-10 Li 2 O 2-6 Na 2 O 0-2 K 2 O 0-2 B 2 O 3 0-1 MgO 0-4 ZnO 0-5 CaO 0-4 BaO 0-5 TiO 2…
The pharmaceutical packing device has a hollow plastic body ( 1 ) of axial length (I) and a cylindrical portion ( 7 ) extending over at least a part of its axial length and an interior silicone lubricant layer ( 3 ) provided on an interior surface of the plastic body in the…
The invention provides a lithium-free boron alumino-silicate glass composition which is chemically toughened and a glass article manufactured thereof. The glass article has a CTE lower than 7.5 ppm/K -1 at a temperature of 20 to 300°C, a Dol higher than 10 μm and a CS higher…