Schmidtgen Ulf
A lamellar graphite cast iron alloy is described which, as additives, has 2.80% by weight-3.60% by weight carbon (C), 1.00% by weight-1.70% by weight silicon (Si), 0.10% by weight-1.20% by weight manganese (Mn), 0.03% by weight-0.15% by weight sulphur (S), 0.05% by weight-0.30%…
The invention relates to a cast iron alloy having lamellar graphite and comprising 2.80 wt % - 3.60 wt % carbon (C), 1.00 wt % - 1.70 wt % silicon (Si), 0.10 wt % - 1.20 wt % manganese (Mn), 0.03 wt % - 0.15 wt % sulfur (S), 0.05 wt % - 0.30 wt % chromium (Cr), 0.05 wt % - 0.30…
The invention relates to a method for producing a tape-wound toroidal core, comprising the steps of: • providing a soft-magnetic tape (1) on at least two tape reels (3), • unwinding the tape (1) from two tape reels (3) and winding the tape (1) onto two winding mandrels (5),…
A method for producing a tape-wound toroidal core includes: ⋅providing a soft-magnetic tape on two tape reels, ⋅unwinding the tape and winding the tape onto two winding mandrels to form a multilayer first tape roll, wherein, after in each case several layers, a separating plate…
The invention relates to a method for producing a tape-wound toroidal core, comprising the steps of: • providing a soft-magnetic tape (1) on at least two tape reels (3), • unwinding the tape (1) from two tape reels (3) and winding the tape (1) onto two winding mandrels (5),…