Patents
Assignee / Organization

Sagara Masayuki

63Total Forward Citations
12Indexed Patents
5Avg Citations / Patent
6Portfolio H-Index
WO 2010/113843 A1#9021754 Most Cited · 11 citations0.7/yr · PR 2.85PendingWO · Application
Method for producing high-strength seamless cr-ni alloy pipe

Disclosed is a method for producing a high-strength seamless Cr-Ni alloy pipe which has excellent hot workability and stress corrosion cracking resistance while having high strength by increasing the content of nitrogen, and does not cause cracking into two pieces during…

US 2010170320 A1#9956003 Most Cited · 10 citations0.6/yr · PR 3.03PendingUS · Application
Method for manufacturing a high alloy pipe

A method for manufacturing a high alloy pipe comprises hot working, a high alloy material pipe having controlled amounts of C, Si, Mn, P, S, Ni, Cr, Mo, Cu, Al, N, O, and optionally Ca, Mg, and rare earth elements, with the balance Fe. The pipe composition satisfies the formula…

US 2006201587 A1#11844438 Most Cited · 9 citations0.5/yr · PR 1.91PendingUS · Application
Welded structure having improved resistance to stress corrosion cracking

This invention relates to a welded line pipe structure for transporting corrosive petroleum or natural gas. It is constituted by martensitic stainless steel pipes containing 8-16% Cr and at most 0.05% C. By suitably controlling the welding conditions at the time of girth welding…

WO 2005/023478 A1#12821638 Most Cited · 8 citations0.4/yr · PR 2.31PendingWO · Application
Welded structure excellent in resistance to stress corrosion cracking

A welded line pipe structure for use in transporting petroleum and a natural gas being corrosive, which comprises a martensitic stainless steel containing 8 to 16 % of Cr and 0.05 % or less of C, wherein a portion reduced in the content of grain boundary Cr being located…

WO 2009/150989 A1#17100531 Most Cited · 6 citations0.3/yr · PR 1.86PendingWO · Application
Process for producing high-alloy seamless pipe

A work to be extruded which comprises a high alloy containing, in terms of mass%, 20-30% chromium and 22-60%, excluding 22%, nickel is hot-extruded while being heated, according to the contents of molybdenum and tungsten, to a heating temperature T (°C) satisfying the…

WO 9,909,231 A1#16565413 Most Cited · 6 citations0.2/yr · PR 2.39PendingWO · Application
Austenitic stainless steel excellent in resistance to sulfuric acid corrosion and workability

An austenitic stainless steel which consists, on a weight basis, of up to 0.05 % carbon, up to 1.0 % silicon, up to 2.0 % manganese, up to 0.04 % phosphorus, up to 0.01 % sulfur, 12-27 % nickel, 15-26 % chromium, 3.0-8.0 %, excluding 3.0 %, copper, 2.0-5.0 %, excluding 2.0 %,…

US 2009081069 A1#33194291 Most Cited · 3 citations0.2/yr · PR 1.05PendingUS · Application
Austenitic stainless steel

An austenitic stainless steel, which comprises by mass percent, C: not more than 0.10%, Si: 0.01 to 1.0%, Mn: 0.01 to 2%, Cr: 16 to 18%, Ni: more than 10% to less than 14%, Mo: more than 2.0% to not more than 3.0%, N: 0.03 to 0.10%, one or more elements selected from V, Nb and…

US 2012031534 A1#28948567 Most Cited · 3 citations0.2/yr · PR 1.39PendingUS · Application
METHOD FOR PRODUCING HIGH-STRENGTH Cr-Ni ALLOY SEAMLESS PIPE

A method for producing a high-strength Cr—Ni alloy seamless pipe comprising preparing an alloy billet with a chemical composition consisting, by mass %, of C: 0.05% or less, Si: 1.0% or less, Mn: less than 3.0%, P: 0.005% or less, S: 0.005% or less, Cu: 0.01 to 4.0%, Ni: 25% or…

WO 2007/138815 A1#30352114 Most Cited · 3 citations0.2/yr · PR 1.22PendingWO · Application
Austenitic stainless steel

An austenitic stainless steel which contains, by mass, C: 0.10% or below, Si: 0.01 to 1.0%, Mn: 0.01 to 2%, Cr: 16 to 18%, Ni: more than 10% and less than 14%, Mo: more than 2.0% and up to 3.0%, N: 0.03 to 0.10%, and one or more of V, Nb and Ti in amounts satisfying the…

US 8,701,455 B2#40397295 Most Cited · 2 citations0.2/yr · PR 1.00ActiveUS · Utility
Method for manufacturing a high alloy pipe

A method for manufacturing a high alloy pipe comprises hot working, a high alloy material pipe having controlled amounts of C, Si, Mn, P, S, Ni, Cr, Mo, Cu, Al, N, O, and optionally Ca, Mg, and rare earth elements, with the balance Fe. The pipe composition satisfies the formula…

US 8,245,552 B2#61910044 Most Cited · 1 citations0.1/yr · PR 0.74ActiveUS · Utility
Process for producing high-alloy seamless tube
Inventors: Murakami Hiroaki, Yamakawa Tomio, Douhara Tadashi, Sagara MasayukiAssignee: Murakami Hiroaki, Yamakawa TomioFiled 2010-11-24 · Granted 2012-08-21

A starting material to be extruded made of a high alloy comprising, in mass %, Cr: 20 to 30% and Ni: more than 22% and 60% or less is heated to a temperature predetermined according to the contents of Mo and W and is subjected to a hot-extrusion process, the heating temperature…

WO 2009/004970 A1#49498361 Most Cited · 1 citations0.1/yr · PR 0.89PendingWO · Application
Process for production of high alloy steel pipe

The invention provides a process for the production of a high alloy steel which permits pipe making by hot working and which exhibits satisfactory ductility in cold working conducted after pipe making for the purpose of attaining higher strength and is excellent in corrosion…