A method for bending radiation shielding glass which has a heavy metal oxide content of at least 50% by weight is provided, wherein first a mold is provided, a glass plate comprising a radiation shielding glass is then provided, the mold is preheated to a temperature of 300 to…
Assignee / Organization
Roessler Dirk
19Total Forward Citations
3Indexed Patents
6Avg Citations / Patent
2Portfolio H-Index
A method for bending radiation shielding glass which has a heavy metal oxide content of at least 50% by weight is provided, wherein first a mold is provided, a glass plate comprising a radiation shielding glass is then provided, the mold is preheated to a temperature of 300 to…
The invention relates to a method for producing a two or three dimensional glass body. In order to increase mechanical and thermical resistance the rough glass body is produced in the following manner: a rough glass body is produced; said rough body is heated and raised to a…