In a method for increasing the strength of a component subjected to torsional and flexural stress, in particular of a crankshaft, in a first step essentially the entire component is provided with a nitriding layer. In a second step, the nitriding layer is at least partially…
Reeb Alfons
The invention relates to a method for increasing the bending strength and the endurance limit of crankshafts by locally restricted hammering in areas of high stress, such as grooves, the mouths of bores and cross-sectional transition zones, in which method pressure impulse…
In a method for increasing the strength of a component subjected to torsional and flexural stress, in particular of a crankshaft, in a first step essentially the entire component is provided with a nitriding layer. In a second step, the nitriding layer is at least partially…
Disclosed is a method for hardening fillets of a shaft (1), especially a crankshaft (1). According to said method, at least some of the fillets (3) are hardened at bearing points of the shaft (1) in a hardening process comprising inductive hardening by means of at least one…
The invention relates to a method for increasing the bending strength and the endurance limit of crankshafts by locally restricted hammering in areas of high stress, such as grooves, the mouths of bores and cross-sectional transition zones, in which method pressure impulse…
Disclosed is a method for increasing the strength of a part, especially a crankshaft, which is subject to torsional and bending stress. In said method, essentially the entire part is provided with a nitride layer in a first step, the nitride layer is at least partially removed…
In a method for introducing transition radii into a crankshaft (1) between crank pins (2) and crank webs (3) and/or between the bearing pins and crank webs, wherein the contour profile of the transitions (5) between the crank webs (3), the crank pins (2) and bearings (4) of the…
Disclosed is a method for increasing the strength of a part, especially a crankshaft, which is subject to torsional and bending stress. In said method, essentially the entire part is provided with a nitride layer in a first step, the nitride layer is at least partially removed…