A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a t g of 95°C or greater and having a melt processing temperature of 250°C or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an…
Assignee / Organization
Polymer Dynamix Inc
0Total Forward Citations
3Indexed Patents
0Avg Citations / Patent
0Portfolio H-Index
A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a t g of 95°C or greater and having a melt processing temperature of 250°C or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an…
A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a t g of 95°C or greater and having a melt processing temperature of 250°C or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an…