In sophisticated semiconductor devices, a chip-package interconnect structure may be established on the basis of a metal pillar without using a solder bump material in the package. In this case, the complexity of the manufacturing process for forming the wiring system of the…
Platz Alexander
By controlling the cooling rate during the oxidation process for forming an oxide layer on solder balls and by selecting an elevated temperature as an initial temperature of the oxidation process, a reliable yet easily removable oxide layer may be obtained. Consequently, yield…
By directly forming an underbump metallization layer on a contact region of the last metallization layer, the formation of any other terminal metals, such as aluminum and corresponding adhesion/barrier layers, may be avoided. Consequently, the thermal and electrical behavior of…
In a metallization system of a sophisticated semiconductor device, metal pillars may be provided so as to exhibit an increased efficiency in distributing any mechanical stress exerted thereon. This may be accomplished by significantly increasing the surface area of the final…
By patterning the underbump metallization layer stack on the basis of a dry etch process, significant advantages may be achieved compared to conventional techniques involving a highly complex wet chemical etch process. In particular embodiments, a titanium tungsten layer or any…
One illustrative method disclosed herein includes forming a conductive pad in a layer of insulating material, forming a passivation layer above the conductive pad, performing at least one etching process on the passivation layer to define an opening in the passivation layer that…
In a metallization system of a sophisticated semiconductor device, metal pillars 271 may be provided so as to exhibit an increased efficiency in distributing any mechanical stress exerted thereon. This may be accomplished by significantly increasing the surface area of the final…
A die seal of a semiconductor device may be provided with a varying pattern density such that a gradient between the die region and the die seal may be reduced. Consequently, for a given width of the die seal, a required mechanical stability may be achieved, while at the same…
One illustrative method disclosed herein includes forming a conductive pad in a layer of insulating material, forming a passivation layer above the conductive pad, performing at least one etching process on the passivation layer to define an opening in the passivation layer that…
By directly forming an underbump metallization layer (211) on a contact region (202A) of the last metallization layer, the formation of any other terminal metals, such as aluminum and corresponding adhesion/barrier layers, may be avoided. Consequently, the thermal and electrical…
By patterning an underbump metallization layer stack (105) on the basis of a dry etch process (111), significant advantages may be achieved compared to conventional techniques involving a highly complex wet chemical etch process. In particular embodiments, a titanium tungsten…
By patterning an underbump metallization layer stack (105) on the basis of a dry etch process (111), significant advantages may be achieved compared to conventional techniques involving a highly complex wet chemical etch process. In particular embodiments, a titanium tungsten…
By directly forming an underbump metallization layer (211) on a contact region (202A) of the last metallization layer, the formation of any other terminal metals, such as aluminum and corresponding adhesion/barrier layers, may be avoided. Consequently, the thermal and electrical…
In a metallization system of a sophisticated semiconductor device, metal pillars 271 may be provided so as to exhibit an increased efficiency in distributing any mechanical stress exerted thereon. This may be accomplished by significantly increasing the surface area of the final…