A nickel-chromium-molybdenum alloy capable of being age hardened for improved strength while maintaining high corrosion resistance contains in weight percent 19.5 to 22 chromium, 15 to 17.5 molybdenum, up to 3 iron, up to 1.5 manganese, up to 0.5 aluminum, up to 0.02 carbon, up…
Pike Lee
A wrought age-hardenable nickel-chromium-cobalt based alloy suitable for use in high temperature gas turbine transition ducts possessing a combination of three specific key properties, namely resistance to strain age cracking, good thermal stability, and good creep-rupture…
A wrought age-hardenable nickel-chromium-cobalt based alloy suitable for use in high temperature gas turbine transition ducts possessing a combination of three specific key properties, namely resistance to strain age cracking, good thermal stability, and good creep-rupture…
A single step heat treatment for Ni—Cr—Mo alloys containing from 12% to 19% chromium and from 18% to 23% molybdenum provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to…
A two step heat treatment for Ni—Cr—Mo alloys containing from 12% to 23.5% chromium provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to current practices. This treatment is…
A two step heat treatment for Ni—Cr—Mo alloys containing from 12% to 23.5% chromium provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to current practices. This treatment is…
A single step heat treatment for Ni-Cr-Mo alloys containing from 12% to 19% chromium and from 18% to 23% molybdenum provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to…
An alloy designed for use in gas turbine engines which has high strength and a low coefficient of thermal expansion is disclosed. The alloy may contain in weight percent 7% to 9% chromium, 21% to 24% molybdenum, greater than 5% tungsten, up to 3% iron, with a balance being…
An alloy designed for use in gas turbine engines which has high strength and a low coefficient of thermal expansion is disclosed. The alloy may contain in weight percent 7% to 9% chromium, 21% to 24% molybdenum, greater than 5% tungsten, up to 3% iron, with a balance being…
An alloy designed for use in gas turbine engines which has high strength and a low coefficient of thermal expansion is disclosed. The alloy may contain in weight percent 7% to 9% chromium, 21% to 24% molybdenum, greater than 5% tungsten, up to 3% iron, with a balance being…