Patents
Assignee / Organization

Petrecycle Ltd

5Total Forward Citations
10Indexed Patents
0Avg Citations / Patent
1Portfolio H-Index
US 7,214,723 B2#26988950 Most Cited · 4 citations0.2/yr · PR 1.13ExpiredUS · Utility
Method for the decontamination of polyethylene terephthalate
Inventors: West Simon MichaelAssignee: Petrecycle LtdFiled 2004-02-27 · Granted 2007-05-08

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

WO 2005/079140 A2#59968576 Most Cited · 1 citations0.1/yr · PR 0.77PendingWO · Application
A method for the decontamination of polyethylene terephthalate
Inventors: West Simon MichaelAssignee: Petrecycle LtdFiled 2004-02-27

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

CN 100,503,700 C#140311844 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
A method for the decontamination of polyethylene terephthalate
Inventors: Michael West SimonAssignee: Petrecycle LtdFiled 2004-02-27 · Granted 2009-06-24

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

CN 1,863,855 A#109662275 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
A method for the decontamination of polyethylene terephthalate
Inventors: Michael West SimonAssignee: Petrecycle LtdFiled 2004-02-27

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

EP 1,603,861 A2#89587066 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
A method for the decontamination of polyethylene terephthalate
Inventors: West Simon MichaelAssignee: Petrecycle LtdFiled 2004-02-27

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

EP 1,603,861 A4#102669617 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
A method for the decontamination of polyethylene terephthalate
Inventors: West Simon MichaelAssignee: Petrecycle LtdFiled 2004-02-27

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…

WO 2005/079140 A3#93516276 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
A method for the decontamination of polyethylene terephthalate
Inventors: West Simon MichaelAssignee: Petrecycle LtdFiled 2004-02-27

A process for removing contaminants from PET components by mixing ethanediol with the PET feedstock at a temperature about the boiling point of ethanediol and for a time sufficient to convert the polyethylene terephthate components to polyethylene terephthate polymers which are…