A shaped part having at least two structural regions of different ductility is made from one unitary blank of a hardenable steel alloy by first heating the entire blank to an elevated temperature below an AC 3 point of the alloy. Then only first regions of the blank are heated…
Pellmann Markus
A blank cut from a strip of hardenable hot-formed steel is heated in a furnace to a temperature which is smaller than an Ac 3 transformation point in an iron carbon diagram. A first region of the blank is then heated in a conductive heating station to a temperature above the Ac…
The present invention relates to a method for producing a hot-formed and press-hardened metal component for an automobile having at least two regions of different hardness. A hardenable sheet-metal blank is heated to at least an austenizing temperature and a first region of the…
An automobile column and to a method for producing an automobile column are disclosed. The automobile column has a region of a first type and a region of a second type which have mutually different strengths. A transition region having a width of less than 50 mm is formed…
A blank cut from a strip of hardenable hot-formed steel is heated in a furnace to a temperature which is smaller than an Ac 3 transformation point in an iron carbon diagram. A first region of the blank is then heated in a conductive heating station to a temperature above the Ac…
Method for producing an open molded sheet metal part from a non-hardenable aluminum alloy that has the following steps: a) a sheet is prepared that is made of a non-hardenable aluminum alloy, the temper of which is H12, H14, H16, H18, H19, H22, H24, H26, H28, H32, H34, H36 or…
In a method of producing a hardened formed part, in particular for a structure or body part of a motor vehicle, a metal blank is heated and then hot formed in a cavity of a thermoforming mold to produce a formed part. The formed part is hardened in the cavity of the…
A side rail and to a method for producing a side rail are disclosed. The side rail has a region of a first type and a region of a second type which have mutually different strengths. A transition region having a width of less than 50 mm is formed between the two regions. The…
In a method for producing in particular structural components or chassis components for a motor vehicle by hot or semi-hot forming, a sheet metal blank is heated in a heating station at least in a first region from a starting temperature to a target temperature, and then the…
A method for producing a structural and/or safety-related motor vehicle component having at least one hot-formed and press-hardened part constructed from high-strength steel includes the steps of partially heat-treating a region of the motor vehicle component by heating the…
According to the method, a printed circuit board (7) that is severed from the strip material (4) comprising coated, high-strength boron steel is homogeneously heated in a furnace (11) having a plurality of temperature zones (8, 9, 10) first in a first zone (8) to a temperature…
The present invention relates to a method for producing a hot-formed and press-hardened metal component for an automobile having at least two regions of different hardness. A hardenable sheet-metal blank is heated to at least an austenizing temperature and a first region of the…
On a body structure ( 2 ) for an automobile ( 1 ) having a structural component ( 3 ) made of at least high-strength steel sheet, the structural component ( 3 ) is provided with a predetermined cutting location ( 5, 5 a, 5 b, 5 c ) for applying a separating tool. In the method…
In a method for producing in particular structural components or chassis components for a motor vehicle by hot or semi-hot forming, a sheet metal blank is heated in a heating station at least in a first region from a starting temperature to a target temperature, and then the…
There is described a method for producing press-hardened shaped components, in particular bodywork or structural components of motor vehicles. The shaped components are produced from blanks (4) of hot-forming steel, for which purpose the blanks (4) are heated in a liquid bath…
There is described a method for producing press-hardened shaped components, in particular bodywork or structural components of motor vehicles. The shaped components are produced from blanks (4) of hot-forming steel, for which purpose the blanks (4) are heated in a liquid bath…
The invention relates to the production in particular of structural components or chassis components (14) for a motor vehicle by hot or semi-hot forming, wherein a sheet metal blank is heated in a heating station (1) at least in a first region from a starting temperature to a…