An alloy suitable for use in a ball grid array, the alloy comprising from 0.15 - 1.5 wt.% copper, from 0.1 - 4 wt.% silver, from 0 - 0.1 wt.% phosphorus, from 0 - 0.1 wt.% germanium, from 0 - 0.1 wt.% gallium, from 0 - 0.3 wt.% of one or more rare earth elements, from 0 - 0.3…
Pandher Ranjit
High Impact Toughness Alloy The invention provides an alloy, preferably a lead-free solder alloy, comprising: from 35 to 59 %wt Bi; from 0 to.0 wt% Ag; from 0 to 1.0 %wt Au; from 0 to 1.0 %wt Cr; from 0 to 2.0 %wt In; from 0 to 1.0 %wt P; from 0 to 1.0 %wt Sb; from 0 to 1.0 %wt…
High Impact Toughness Alloy The invention provides an alloy, preferably a lead-free solder alloy, comprising: from 35 to 59% wt Bi; from 0 to 0.0 wt % Ag; from 0 to 1.0% wt Au; from 0 to 1.0% wt Cr; from 0 to 2.0% wt In; from 0 to 1.0% wt P; from 0 to 1.0% wt Sb; from 0 to 1.0%…
An alloy suitable for use in a wave solder process, reflow soldering process, hot air levelling process or a ball grid array, the alloy comprising from 0.08 - 3 wt.% bismuth, from 0.15 - 1.5 wt.% copper, from 0.1 - 1.5 wt.% silver, from 0 - 0.1 wt.% phosphorus, from 0 - 0.1 wt.%…
A solder composition comprising a blend of a first powder component and a second powder component, wherein the first powder component is a first solder alloy and the second powder component is a second solder alloy or a metal.
A solder composition comprising a blend of a first powder component and a second powder component, wherein the first powder component is a first solder alloy and the second powder component is a second solder alloy or a metal.
A method for curing polymerizable compositions by irradiating the compositions with a pulsed light that is emitted from an LED. The method of the present invention is especially suitable for curing dental compositions.
In the manufacture of products such as printed wiring boards or chip scale packaging and ball grid arrays, incorporating one or more elements selected from among Ni, Co, Cr, Mn, Zr, Fe and Si into a lead-free soldering process to reduce joint embrittlement. In varied embodiments…
An alloy suitable for use in a wave solder process, reflow soldering process, hot air levelling process or a ball grid array, the alloy comprising from 0.08-3 wt. % bismuth, from 0.15-1.5 wt. % copper, from 0.1-1.5 wt. % silver, from 0-0.1 wt. % phosphorus, from 0-0.1 wt. %…
An alloy suitable for use in a ball grid array or chip scale package comprising from 0.05-1.5 wt. % copper, from 0.1-2 wt. % silver, from 0.005-0.3 wt % nickel, from 0.003-0.3 wt % chromium, from 0-0.1 wt. % phosphorus, from 0-0.1 wt. % germanium, from 0-0.1 wt. % gallium, from…
An alloy suitable for use in a ball grid array, the alloy comprising from 0.15 - 1.5 wt.% copper, from 0.1 - 4 wt.% silver, from 0 - 0.1 wt.% phosphorus, from 0 - 0.1 wt.% germanium, from 0 - 0.1 wt.% gallium, from 0 - 0.3 wt.% of one or more rare earth elements, from 0 - 0.3…
A solder composition comprising a blend of a first powder component and a second powder component, wherein the first powder component is a first solder alloy and the second powder component is a second solder alloy or a metal.
A method of forming a solder joint, comprising: (a) providing a lead-free, tin-containing solder alloy; (b) providing a printed wiring board substrate or a ball grid array substrate, said substrate being formed from a material comprising copper, optionally also zinc, and one or…