A sputtering target with an integrated backing plate characterized in that the Vickers hardness (Hv) of a flange part is at least 90, and the 0.2% yield stress of the flange part is at least 6.98×10 7 N/m 2 . By increasing the mechanical strength of only the flange part of the…
Otsuki Tomio
Provided is a high-purity copper-manganese-alloy sputtering target comprising 0.05 to 20 wt. % of Mn, 2 wt ppm or less of C, and the remainder being Cu and inevitable impurities, wherein in formation of a film on a wafer by sputtering the target, the number of particles composed…
Provided are a lanthanum target for sputtering which has a recrystallized structure with an average crystal grain size of 100 μm or less and has no spotty macro patterns on the surface; and a method of producing a lanthanum target for sputtering, wherein lanthanum is melted and…
A backing plate integrated sputtering target includes a flange part having a Vicker's hardness (Hv) of 90 or more and a 0.2% yield stress of 6.98×10 7 N/m 2 or more. Enhancing the mechanical strength of only the flange part of the target inhibits the target from being…
Provided are a lanthanum target for sputtering which has a Vickers hardness of 60 or more and no spotty macro patterns on the surface, and a method of producing a lanthanum target for sputtering, wherein lanthanum is melted and cast to produce an ingot, the ingot is subject to…
[Abstract] A high-purity copper-manganese-alloy sputtering target containing 0.05-20 wt% of Mn and 2 wt ppm or less of C, the balance being constituted by Cu and inevitable impurities, wherein the high-purity copper-manganese-alloy sputtering target is characterized in that when…
The object of this invention is to provide a high quality titanium target for sputtering capable of reducing the impurities that cause generation of particles and abnormal discharge, which is free from fractures and cracks during high power sputtering (high rate sputtering), and…
Provided is a high-purity copper-manganese-alloy sputtering target comprising 0.05 to 20 wt % of Mn and the remainder being Cu and inevitable impurities. The high-purity copper-manganese-alloy sputtering target is characterized in that the in-plane variation (CV value) in Mn…
A copper-titanium alloy sputtering target comprising 3 at % or more and less than 15 at % of Ti and a remainder made up of Cu and unavoidable impurities, wherein a variation (standard deviation) in hardness is within 5.0 and a variation (standard deviation) in electric…
Provided is a high-purity copper-manganese-alloy sputtering target comprising 0.05 to 20 wt % of Mn and the remainder being Cu and inevitable impurities. The high-purity copper-manganese-alloy sputtering target is characterized in that the in-plane variation (CV value) in Mn…
A copper-titanium alloy sputtering target comprising 3 at% or more and less than 15 at% of Ti and a remainder made up by Cu and unavoidable impurities, and characterized in that the deviation (standard deviation) of the values of hardness is within ± 5.0 and the deviation…
[Abstract] A high-purity copper-manganese-alloy sputtering target containing 0.05-20 wt% of Mn, with Cu and inevitable impurities constituting the balance, wherein the high-purity copper-manganese-alloy sputtering target is characterized in that the in-plane variation (CV value)…
The object of this invention is to provide a high quality titanium target for sputtering capable of reducing the impurities that cause generation of particles and abnormal discharge, which is free from fractures and cracks during high power sputtering (high rate sputtering), and…
A lanthanum target for sputtering which has a Vickers hardness of 60 or higher and has no macroscopic spot in the surface. A process for producing a lanthanum target for sputtering is provided which is characterized by melting and casting lanthanum to produce an ingot, forging…
A backing plate integrated sputtering target includes a flange part having a Vicker's hardness (Hv) of 90 or more and a 0.2% yield stress of 6.98×10 7 N/m 2 or more. Enhancing the mechanical strength of only the flange part of the target inhibits the target from being…
Provided are a lanthanum target for sputtering which has a Vickers hardness of 60 or more and no spotty macro patterns on the surface, and a method of producing a lanthanum target for sputtering, wherein lanthanum is melted and cast to produce an ingot, the ingot is subject to…
Provided are a lanthanum target for sputtering which has a recrystallized structure with an average crystal grain size of 100 μm or less and has no spotty macro patterns on the surface; and a method of producing a lanthanum target for sputtering, wherein lanthanum is melted and…
A lanthanum target for sputtering which has a recrystallized structure with an average crystal grain diameter of 100 µm or smaller and has no macroscopic spot in the surface. A process for producing a lanthanum target for sputtering is provided which is characterized by melting…