Patents
Assignee / Organization

Ota Mie

52Total Forward Citations
8Indexed Patents
6Avg Citations / Patent
4Portfolio H-Index
US 2013324629 A1#6406187 Most Cited · 15 citations1.1/yr · PR 2.34PendingUS · Application
Resin foam and process for producing the same

Provided is a resin foam which has satisfactory strain recovery, is particularly resistant to shrinkage of its cell structure caused by the resinous restitutive force at high temperatures, and exhibits superior high-temperature strain recovery. The resin foam according to the…

WO 2013/018582 A1#6812109 Most Cited · 14 citations1.1/yr · PR 2.92PendingWO · Application
Resin foam and manufacturing method therefor

Provided is a resin foam having excellent dust resistance, even at high temperatures. The resin foam according to the first embodiment of the present invention is characterized by having a thickness recovery rate (23°C, 1 minute, 50% compression), as defined below, of at least…

WO 2012/111443 A1#8919734 Most Cited · 11 citations0.8/yr · PR 3.28PendingWO · Application
Resin foam and production method therefor

Provided is a resin foam having excellent strain recovery, in particular having little shrinkage of the foam structure at high temperatures caused by the recovery force of the resin and excellent strain recovery at high temperatures. This resin foam is characterized by: being…

US 2014155507 A1#24060578 Most Cited · 4 citations0.3/yr · PR 1.49PendingUS · Application
Resin foam and process for producing the same

Provided is a resin foam that is satisfactorily flexible and highly resistant to heat, exhibits superior strain recoverability at high temperatures, and has a high instantaneous recovery rate. This resin foam is formed from a resin composition containing an acrylic polymer, an…

US 2013075958 A1#28510393 Most Cited · 3 citations0.2/yr · PR 1.49PendingUS · Application
Process for producing thermoplastic resin foam

The present invention provides a process for producing a thermoplastic resin foam excellent in strength, flexibility, cushioning properties, strain recovery, and appearance, and exhibiting little shrinkage of the cell structure under a high temperature condition and a high…

US 2014170406 A1#45284345 Most Cited · 2 citations0.2/yr · PR 0.87PendingUS · Application
Resin foam and process for producing the same

A resin foam has a thickness recovery rate (23° C., one minute, 50% compression) of 70% or more and a strain recovery rate (80° C., 24 hours, 50% compression) of 80% or more. The thickness recovery rate is determined by compressing the resin foam, holding the resin foam in the…

WO 2013/018581 A1#38053782 Most Cited · 2 citations0.1/yr · PR 1.07PendingWO · Application
Resin foam and manufacturing method therefor

Provided is a resin foam having excellent flexibility, heat resistance, strain recovery under high temperatures, and an excellent instantaneous recovery rate. This resin foam is characterized in that said resin foam is formed using a resin composition including an acrylic…

JP 2000258561 A#57505306 Most Cited · 1 citations0.0/yr · PR 0.79ExpiredJP · Utility
Clock using disk-shaped storage medium and spacer
Inventors: Ota MieAssignee: Ota MieFiled 1999-03-11

PROBLEM TO BE SOLVED: To obtain a clock using a disk-shaped storage medium that can be easily created such as a CD and a CD-ROM as the dial of the clock. SOLUTION: A clock movement 3 is arranged on the back surface of a CD1, and an electronic clock hand shaft 3a is allowed to…