Patents
US 6,267,829 B1#1440156 Most Cited · 39 citations1.6/yr · PR 9.18ExpiredUS · Utility
Method of reducing the formation of primary platelet-shaped beta-phase in iron containing alSi-alloys, in particular in Al-Si-Mn-Fe alloys
Inventors: Baeckerud Lennart, Arnberg Lars, Chai GuocaiAssignee: Opticast AbFiled 1996-10-09 · Granted 2001-07-31

The present invention is a method for producing an iron-containing hypoeutectic alloy free from primary platelet-shaped beta-phase of the Al 5 FeSi in the solidified structure by the steps (a) providing an iron-containing aluminum alloy having a composition within the following…

WO 9,713,882 A1#6142459 Most Cited · 15 citations0.5/yr · PR 3.57PendingWO · Application
A METHOD OF REDUCING THE FORMATION OF PRIMARY PLATLET-SHAPED BETA-PHASE IN IRON CONTAINING AlSi-ALLOYS, IN PARTICULAR IN Al-Si-Mn-Fe ALLOYS

Iron is a detrimental impurity in aluminium alloys since it causes hard and brittle iron-rich intermetallic phases to precipitate during solidification. The most detrimental phase in the microstructure is the beta-phase of the Al5FeSi-type because it is platelet-shaped. The…

US 6,073,677 A#11632361 Most Cited · 9 citations0.3/yr · PR 2.09ExpiredUS · Utility
Method for optimization of the grain refinement of aluminum alloys
Inventors: Baeckerud Lennart, Johnsson Mats, Sigworth GeoffreyAssignee: Opticast AbFiled 1996-11-21 · Granted 2000-06-13

The invention is a method of controlling the grain refinement of certain aluminium alloys. The grain sizes for different values of the grain growth index, GGI, are determined for the used casting method. The GGI is represented by the sum of m(k-1) value multiplied with the…

EP 0,859,868 A1#24239309 Most Cited · 4 citations0.1/yr · PR 1.46PendingEP · Application
A METHOD OF REDUCING THE FORMATION OF PRIMARY PLATLET-SHAPED BETA-PHASE IN IRON CONTAINING AlSi-ALLOYS, IN PARTICULAR IN Al-Si-Mn-Fe ALLOYS
Inventors: Baeckerud Lennart, Arnberg Lars, Chai GuocaiAssignee: Opticast AbFiled 1996-10-09

Iron is a detrimental impurity in aluminium alloys since it causes hard and brittle iron-rich intermetallic phases to precipitate during solidification. The most detrimental phase in the microstructure is the beta-phase of the Al5FeSi-type because it is platelet-shaped. The…

WO 9,719,200 A1#23640469 Most Cited · 4 citations0.1/yr · PR 1.60PendingWO · Application
Improved method for optimization of the grain refinement of aluminium alloys

The invention is a method of controlling the grain refinement of certain aluminium alloys. The grain sizes for different values of the grain growth index, GGI, are determined for the used casting method. The GGI is represented by the sum of m(k - 1) value multiplied with the…

EP 0,866,882 A1#43935444 Most Cited · 2 citations0.1/yr · PR 0.92PendingEP · Application
Improved method for optimization of the grain refinement of aluminium alloys

The invention is a method of controlling the grain refinement of certain aluminium alloys. The grain sizes for different values of the grain growth index, GGI, are determined for the used casting method. The GGI is represented by the sum of m(k - 1) value multiplied with the…

CA 2,234,094 A1#50144752 Most Cited · 1 citations0.0/yr · PR 0.86PendingCA · Application
A method of reducing the formation of primary platelet-shaped beta-phasein iron containing alsi-alloys, in particular in al-si-mn-fe alloys
Inventors: Arnberg Lars, Chai Guocai, Baeckerud LennartAssignee: Opticast AbFiled 1996-10-09

Iron is a detrimental impurity in aluminium alloys since it causes hard and brittle iron-rich intermetallic phases to precipitate during solidification. The most detrimental phase in the microstructure is the beta-phase of the Al5FeSi-type because it is platelet-shaped. The…

CA 2,236,144 A1#49714853 Most Cited · 1 citations0.0/yr · PR 0.88PendingCA · Application
Improved method for optimization of the grain refinement of aluminium alloys

The invention is a method of controlling the grain refinement of certain aluminium alloys. The grain sizes for different values of the grain growth index, GGI, are determined for the used casting method. The GGI is represented by the sum of m(k - 1) value multiplied with the…

BR 9,610,978 A#133940316 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredBR · Utility
Método para reduzir a formação de fase beta em forma de plaqueta primária em ligas de alsi contendo ferro, em particular em ligas de al-si-mn-fe
Inventors: Backerud Lennart, Arnberg Lars, Chai GuocaiAssignee: Opticast AbFiled 1996-10-09

"MéTODO PARA REDUZIR A FORMAçãO DE FASE BETA EM FORMA DE PLAQUETA PRIMáRIA EM LIGAS DE ALSi CONTENDO FERRO, EM PARTICULAR EM LIGAS DE AL-Si-Mn-Fe". O ferro é uma impureza nociva nas ligas de alumínio, uma vez que ele faz com que as fases intermetálicas ricas em ferro…

BR 9,611,467 A#118047189 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredBR · Utility
Método aperfeiçoado para otimização do refinamento de grão de ligas de alumìnio.

''MéTODO APERFEIçOADO PARA OTIMIZAçãO DO REFINAMENTO DE GRãO DE LIGAS DE ALIMìNIO''. Trata-se de um método de controle do refinamento de grãos de certas ligas de alimínio. Os tamanhos de grãos para diferentes valores do índice de crescimento de grãos, GGI, são…

CA 2,236,144 C#148364030 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Improved method for optimization of the grain refinement of aluminium alloys
Inventors: Johnsson Mats, Backerud Stig Lennart, Sigworth Geoffrey KAssignee: Opticast AbFiled 1996-11-21 · Granted 2005-04-26

The invention is a method of controlling the grain refinement of certain aluminium alloys. The grain sizes for different values of the grain growth index, GGI, are determined for the used casting method. The GGI is represented by the sum of m(k - 1) value multiplied with the…

ES 2,145,489 T3#152878753 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Un metodo para reducir la formacion de fase beta primaria, con forma de laminillas, en aleaciones de alsi que contienen hierro, en particular en aleaciones de al-si-mn-fe.
Inventors: Backerud Lennart, Arnberg Lars, Chai GuocaiAssignee: Opticast AbFiled 1996-10-09 · Granted 2000-07-01

EL HIERRO CONSTITUYE UNA IMPUREZA PERJUDICIAL EN LAS ALEACIONES DE ALUMINIO, YA QUE ORIGINA FASES INTERMETALICAS RICAS EN HIERRO QUE SON DURAS Y QUEBRADIZAS Y QUE PRECIPITAN DURANTE LA SOLIDIFICACION. LA FASE MAS PERJUDICIAL QUE SE PRESENTA EN LA MICROESTRUCTURA ES LA FASE BETA…

ES 2,155,210 T3#68971035 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Metodo mejorado para la optimizacion del afino de granos de aleaciones de aluminio.
Inventors: Backerud Stig Lennart, Johnsson Mats, Sigworth GeoffreyAssignee: Opticast AbFiled 1996-11-21 · Granted 2001-05-01

LA INVENCION ES UN PROCEDIMIENTO PARA CONTROLAR EL REFINAMIENTO DE GRANO DE CIERTAS ALEACIONES DE ALUMINIO. SE DETERMINAN LOS TAMAÑOS DE GRANO PARA VALORES DIFERENTES DEL INDICE DE CRECIMIENTO DEL GRANO (GGI) PARA EL PROCEDIMIENTO DE MOLDEO UTILIZADO. EL GGI SE REPRESENTA POR LA…

SE 505,823 C2#114052673 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredSE · Utility
Förfarande för framställning av järninnehållande aluminiumlegeringar fria från flakformad fas av Al5FeSi-typ
Inventors: Baeckerud Lennart, Arnberg Lars, Chai GuocaiAssignee: Opticast AbFiled 1995-10-10

The present invention is a method for producing an iron-containing hypoeutectic alloy free from primary platelet-shaped beta-phase of the Al5FeSi in the solidified structure by the steps (a) providing an iron-containing aluminum alloy having a composition within the following…