Disclosed is a both-side friction stir bonding method wherein a bonding strength is increased and the reliability of the bonding strength is enhanced by minimizing fracture and poor bonding of a metal plate when the metal plate having a thickness smaller than the diameter at the…
Onose Mitsuru
In a cold rolled material production equipment, a strip storage device (50) is provided. The strip storage device (50) is disposed between connection means (23) and rolling machines (10a, 10b). The connection means (23) connects the tail end of a preceding coil (25b), disposed…
In order to perform friction stir welding with excellent economy and high weld strength and reliability, a rotating tool (3) has a tool body (3a) having a shoulder face (3b) formed in the distal end portion thereof and a pin-shaped projection (3d) formed so as to protrude from…
A pair of upper and lower pressure rollers (3, 4) are so arranged that their shaft cores (15, 16) are inclined in directions, within a horizontal face, opposite to a straight line orthogonal to the welding line of a bonding section (J). While driving the pressure rollers (3, 4)…
For a small-to-mid-sized production facility with an annual output between around 300,000 and 600,000 metric tons, the disclosed cold-rolling equipment and method provided an excellent ROI while maintaining high efficiency and yield. Input coils (101a to 101c) paid out from a…
The purpose of the present invention is to prevent the excess increase in temperature of a tool main body in the friction stir welding of a high-melting-point material such as a steel, thereby prolonging the service life of the tool main body. A heat-removing body (4), which is…
Mash seam welding is performed to weld metal plates with thicknesses of 2 mm or more to stabilize the strength of a joint portion, reduce uneven parts of the joint portion, and ensure high strength and reliability of the joint portion. First, two metal plates, clamped with first…
Cold rolled material manufacturing equipment comprises: an unwinding device for unwinding a hot rolled coil after acid pickling; joining means, disposed on the exit side of the unwinding device, for joining the tail end of a preceding coil to the leading end of a succeeding coil…
An apparatus and method of cold rolling for a small sized or medium-sized plant with a capacity from 300thousand to 600 thousand tons of product per year are proposed that have a high efficiency, a high yield and a high cost-efficiency. A strip is directly fed to a cold rolling…
In order to economically perform two-surface friction stir welding resulting in high joint strength, a first and second rotation tool (3, 4) each has a shoulder section (3c, 4c) formed on the tip portion a tool body (3a, 4a). The first rotation tool (3) further has a protrusion…
To perform double-side friction stir welding whereby even when the gap between abutting portions of two metal plates exceeds 0.5 mm, the welding strength is increased by suppressing the welding failure, the economy is improved by suppressing the increase in facility cost, and…
The purpose of the present invention is to perform friction stir joining with improved thermal efficiency without adhesion while preventing an increase in size, enhancing production efficiency, and preventing asymmetric residual stress and unbalanced strength. To this end, a…
In order that in mash seam welding for metal plates with a thickness exceeding 2 mm, the joint strength is stabilized, the difference in the level of a joint part is reduced, high joint strength and reliability are ensured, and therefore metal plates with a thickness exceeding…
In an inspection device for inspecting front and back surfaces of a strip material rolled by a rolling machine, both ends of the strip material along a longitudinal direction of the strip material are claimed by two pairs of clamping devices and the front surface of the back…
A pair of upper and lower electrode rings (1, 2) are arranged such that their axes (17, 18) incline in the opposite directions in a horizontal plane against a line (Y) perpendicularly intersecting a welding line (X) formed at the overlapping portion (L) of two metal plates (5,…
In an inspection device for inspecting front and back surfaces of a strip material rolled by a rolling machine, both ends of the strip material along a longitudinal direction of the strip material are claimed by two pairs of clamping devices and the front surface of the back…
Mash seam welding is performed to weld metal plates with thicknesses of 2 mm or more to stabilize the strength of a joint portion, reduce uneven parts of the joint portion, and ensure high strength and reliability of the joint portion. First, two metal plates, clamped with first…
A pair of upper and lower pressure rollers 3, 4 is disposed so that their axes 15, 16 are tilted in a horizontal plane in respective directions opposite to each other with respect to a straight line perpendicular to a welding line of a joint portion J. The pressure rollers 3, 4…
Disclose is equipment for inspecting the front and back sides of a strip rolled by a rolling machine. Two sets of grippers grip the strip on the both sides in the longitudinal direction, and the front or back side of the strip is pressed at an arbitrary position between the two…