A mixture of styrene and methyl methacrylate in a weight ratio of from 7:3 to 4:6 containing a polymerization initiation is prepolymerized at 70-100 DEG C. for 0.5 to 2 hours, cooled to below 60 DEG C. and on addition of a low boiling foaming agent, a suspension stabilizer and a…
Assignee / Organization
Oldrich Marek
2Total Forward Citations
4Indexed Patents
0Avg Citations / Patent
1Portfolio H-Index
Vinyl polymers are prepared in the form of foamable granules containing volatile foaming agents by partial bulk catalytic polymerization in the absence of foaming agent followed by completion of polymerization in aqueous suspension with a catalyst and a volatile foaming agent at…